Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.50 GPa | 508 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics EXTEM UH1006 TPI Blend High Heat Amorphous TPI Blend, Excellent Chemical Resistance, High Continuous Use Temperature (CUT), Best-in-class FR, OSU and LOI. Material is UL-listed. This material is RoHS compliant and also ha.. |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics EXTEM UH1006 TPI Blend (Asia Pacific) High heat amorphous TPI Blend, Chemical Resistant |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics EXTEM UH1006M TPI Blend High heat amorphous TPI Blend, Chemical Resistant |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics EXTEM UH1006M TPI Blend (Europe-Africa-Middle East) High heat amorphous TPI Blend, Chemical Resistant |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | ISO 527 |
Nilit FRIANYL B63 KG30 Nylon 6 for injection molding, 30% chalk filled Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | ISO 527-1/2 |
Radici Radiflam® AFR (dry) Nylon 66 PA66 Self-extinguishing without halogens or phosphorousInformation provided by Radici group. |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | ISO 527 |
Nilit FRIANYL A63 V2 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, flame retardant, free of halogen and phosphorus.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | ISO 527 |
Nilit FRIANYL B63 W-KV20 Nylon 6 for injection molding, 20% glass ball reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | ASTM D638 |
Manifattura Cattaneo PEEK Polyetheretherketone Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | 1 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 1-3130 30% Talc-Filled Polypropylene Homopolymer INNOPOL® CS 1-3130 is a 30% talc-filled polypropylene homopolymer compound /PP-H TD30 (ISO 1043)/. This grade is available in natural and custom colored form as well.INNOPOL® CS 1-3130 is reco.. |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | ASTM D638 |
Loxim 110 01V0 Polycarbonate, 10% Glass Filled, Flame Retardant Information provided by Loxim Industries |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RAL22S PA 66 (Asia Pacific) LNP* Lubricomp* RAL22S is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 1100R PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM HU1110 PEI Enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem MD130A PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA and EU Food Contact compliant, ISO 10993 compliant in recognized colors.This data was supplied by SABIC-IP for the Europe-.. |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-810 Polyetheretherketone (PEEK) KetaSpire® KT-810 is an ultra-high molecular weight natural PEEK resin having a melt viscosity ranging from 0.51-0.65 kPa-s as compared to 0.38-0.50 kPa-s for standard high-viscosity PEEK grades .. |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-XXXX Polyetheretherketone (PEEK) KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha.. |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | ISO 527 |
Styron CALIBREâ„¢ 7102-8 Polycarbonate CALIBREâ„¢ 7102-8 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBRE.. |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | DIN EN ISO 527 |
Wolf Kunststoff ZEDEX® ZX-324V1T A3H PEEK Polymer, Reinforced Main Characteristics: High resilience; High elasticity; Low permanent deformation; Stress resistant; High strength at temperatures above 140 ° CApplications: Shipbuilding; Chemical Engineering; Aut.. |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | |
Goodfellow Polyhydroxybutyrate - Biopolymer PHB PHB and its copolymers with polyhydroxyvalerate (PHV) are melt-processable semi-crystalline thermoplastics made by biological fermentation from renewable carbohydrate feedstocks. They have been desc.. |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | ISO 527-1/-2 |
DSM Akulon® F223-D Nylon 6 (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 GS 15 HWCP 15% Glass Sphere Filled Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 3.50 GPa | 507 ksi | ASTM D822 |
DuPont Teijin Films Mylar® A Polyester Film, 142 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Tensile Modulus | 3.50 GPa | 507 ksi | ASTM D822 |
DuPont Teijin Films Mylar® A Polyester Film, 75 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | ISO 527-1/-2 |
DSM Akulon® K224-G3 (Cond.) 15% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 3.50 GPa | 507 ksi | ASTM D822 |
DuPont Teijin Films Mylar® A Polyester Film, 750 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Tensile Modulus | 3.50 GPa | 507 ksi | ASTM D822 |
DuPont Teijin Films Mylar® A Polyester Film, 92 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Tensile Modulus | 3.50 GPa | 507 ksi | ASTM D882 |
DuPont Teijin Films Mylar® MDA Polyester Film, 48 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Tensile Modulus | 3.50 GPa | 507 ksi | ASTM D-638 |
Axiall 7777 Rigid PVC, Extrusion Georgia Gulf 7777 is a rigid PVC compound designed for outdoor applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | ISO 527 |
Eurotec® Tecomid® NB40 NL FA50 PA6, unfilled, flame retardant - halogen free, natural Information provided by Eurotec® |