Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.14 GPa | 455 ksi | DIN 53457 |
Isoflon PMMA Polymethyl-methacrylate Products with good mechanical performances under friction and good dimensional stability, notably in moist environmentsVery rigid, hardHigh machining precisionInformation provided by Isoflon. |
|||
Tensile Modulus | 3.14 GPa | 455 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP RX99518 PA 66 LNP* LUBRICOMP* RX99518 is a compound based on PA66 containing Proprietary Fillers. Added feature of this material is: Wear Resistant. |
|||
Tensile Modulus | 3.14 GPa | 455 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Asia Pacific) Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |
|||
Tensile Modulus | 3.14 GPa | 455 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL FP6130 PPE+PS Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |
|||
Tensile Modulus | 3.14 GPa | 455 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Europe-Africa-Middle East) Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |