Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.12 GPa | 453 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion L9630 Polyvinyl Chloride, Rigid (PVC, Rigid) Product can meet UL-94V-0. Material passed V-0 @ 1.5mm in screening test at PDI.Information provided by PolyOne |
|||
Tensile Modulus | 3.12 GPa | 453 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate.. |
|||
Tensile Modulus | 3.12 GPa | 453 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate.. |
|||
Tensile Modulus | 3.12 GPa | 453 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. Internal mold release. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is halogen free.. |
|||
Tensile Modulus | 3.12 GPa | 453 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP FARADEX NS0031 PC+ABS (Asia Pacific) Faradex NS0031 is a compound based on PC+ABS blend resin containing non-brominated and non-chlorinated flame retardant system, Stainless Steel. Added features of this material include: EMI/RFI Shiel.. |
|||
Tensile Modulus | 3.12 GPa | 453 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem AUT230M PEI Transparent polyetherimide (Tg 247 degC). Contains low level of mold release. Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are .. |
|||
Tensile Modulus | 3.12 GPa | 453 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem AUT230M PEI (Asia Pacific) Transparent polyetherimide (Tg 247 degC) with internal mold release. Very low outgassing and plateout for automotive lighting applications where highly metallized, reflective surfaces are required... |
|||
Tensile Modulus | 3.12 GPa | 453 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem AUT230M PEI (Europe-Africa-Middle East) Transparent polyetherimide (Tg 247 degC) with internal mold release. Very low outgassing and plateout for automotive lighting applications where highly metallized, reflective surfaces are required... |
|||
Tensile Modulus | 3.12 GPa | 453 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM XH6050M PEI Copolymer Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Tensile Modulus | 3.12 GPa | 453 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem XH6050M PEI Copolymer (Europe-Africa-Middle East) Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).Thi.. |
|||
Tensile Modulus | 3.12 GPa | 453 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY AX06484 ABS LNP* STAT-LOY* AX06484 is a compound based on ABS resin containing Talc. Added feature of this grade is: Antistatic, Extrudeable. |
|||
Tensile Modulus | 3.12 GPa | 453 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Stat-loy AX06484X ABS LNP* Stat-Loy* AX06484 is a compound based on ABS resin containing mineral filler. Characteristics of this grade is it is extrudeable and static dissipative.This data was supplied by SABIC-IP for t.. |
|||
Tensile Modulus | 3.12 GPa | 453 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM XH6050M PEI Copolymer (Asia Pacific) Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Tensile Modulus | 3.12 GPa | 453 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP DB0049F PC LNP* THERMOCOMP* DB0049F is a compound based on Polycarbonate resin containing 20% Glass Bead. Added features of this material include: Flame Retardant, Superior Molding. |
|||
Tensile Modulus | 3.12 GPa | 453 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP DB0049F PC (Asia Pacific) LNP* Thermocomp* DB0049F is a compound based on Polycarbonate resin containing Glass Bead, Flame Retardant. Added features of this material include: Flame Retardant, Superior Molding. |
|||
Tensile Modulus | 3.12 GPa | 453 ksi | ISO 527 |
Polyram RamTough RZ300G2 Polycarbonate, 10% Glass Fiber 10% Glass fiber reinforced polycarbonate for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 3.12 GPa | 453 ksi | 1 mm/min |
Arkema Group Appryl® HXN 1240 Polypropylene, 40% Talc Filled Compound of a PP homopolymer and 40% talc, warm stabilized suitable for under hood automotive applications.ISO data provided by the manufacturer, Arkema. |