Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.00 GPa | 435 ksi | |
Plastcom SLOVAMID 6 FRM 1 PA6, flame retardant FeaturesDetermined for electrotechnical use. Delivered in natural mode. PA 6 for injection moulding with reduced flammability, with nonhalogen flame retardant. Excellent fluidity of the material pre.. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® C6600 PC+ABS Nonbrominated, nonchlorinated FR PC+ABS with balanced flow, impact and hydrolytic stability for a wide variety of applications including business equipment, monitors, enclosures, among others. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527 |
Nilit FRIANYL A63 CV-CM 0515 9005/Z Powder-coatable nylon 6.6 for injection molding, 15% ceramic filled Powder-coatable nylon 6.6 for injection molding, with conductive carbon blackInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527 |
Nilit FRIANYL B63 F Raw extruded nylon 6 for injection molding Raw extruded nylon 6 for injection molding, highly crystallized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527 |
Nilit FRIANYL B63 KLZ Nylon 6 for injection molding Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ASTM D638 |
Plaskolite West Optix® PL-25 Acrylic Resin Extrusion grade pellets. Highest molecular weight and heat resistance of Optix® line. |
|||
Tensile Modulus | 3.00 GPa @Temperature 23.0 °C |
435 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 988PA NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 988PA NC010 is a low viscosity acetal homopolymer for injection molding with low screw deposit. It is especially formulated for gear applications requiring high precision and dimensional st.. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ASTM D638 |
Fiberfil® PP-60/TC/24/D/HS Polypropylene Homopolymer, Talc Filled, Heat Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem HATX200 PEI+PCE (Asia Pacific) High flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compli.. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | 1 mm/min; ISO 527-1 |
Sax Polymers SAXAMID 226 Nylon 6.6 SAXAMID 226 is a general purpose polyamide 6.6 injection-molding-grade. Benefits are short cycle times and good release properties.Information provided by SAX Polymers |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527-1/-2 |
Unitika A1022GFL15 PA6, 15% Glass Fiber Reinforced, Conditioned Information provided by Unitika Ltd. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | 1mm/min; ISO 527-2/1A |
Topas Advanced Polymers TOPAS® 6017S-04 Cyclic Olefin Copolymer (COC) TOPAS® 6017S-04 is an injection molding grade with a high heat distortion temperature (170°C) and exceptional dimensional stability. It is a glass-clear amorphous polymer with outstanding moisture.. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | DIN 53457/ISO 527 |
Wico Plast Wicotal 130 Acetal ApplicationsInjection moldingAll information provided by Wico Plast, Warenhandelsges. mbH |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527 |
Ecomass® 2150TU96 Tungsten Powder Filled Polyamide (PA6/6), Injection Molding Grade Tungsten Powder Filled Polyamide (PA6/6), Good Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing and radiation shielding applic.. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527-1/-2 |
DSM Akulon® K222-KGMV14 Nylon 6-25% Glass and Mineral Reinforced (European Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527-1/-2 |
DSM Akulon® S227-C Nylon 66 (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® BM-30 PA6-MD30 Product description: Grilon BM-30 is a 30% mineral reinforced PA6 injection moulding grade. Grilon BM-30 has the following important properties: heat stabilizedimpact resistantisotropic shrinkagelig.. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | dry; ISO 527-1/-2 |
DSM Stanyl® TE351 PA46 FR(17) Flame Retardant, Heat Stabilized |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 S Nylon 6, Finely Crystalline, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® FG 40 NL nat 6025 PA6 Product description: Grilon FG 40 NL natural 6025 is a modified, high viscosity polyamide 6. Compared to conventional polyamide 6 Grilon FG40 NL natural 6025 offers the following improvements:Better.. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 327UVE NC010 Acetal (POM)
(Unverified Data**) UV Stabilized Medium-high Viscosity Acetal Homopolymer with Very Low Emissions Delrin 327UVE NC010 (formerly DE20554) is a medium-high viscosity acetal homopolymer with UV stabilizers with very low .. |
|||
Tensile Modulus | 3.00 GPa @Temperature 23.0 °C |
435 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 500PE NC010A Acetal Homopolymer Delrin® 500PE NC010A is a medium viscosity acetal homopolymer, an enhanced version of Delrin® 500P with extremely low VOC emissions. It has improved processing thermal stability, and good mechanic.. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide A28K PA66, Heat Stabilized, Injection Molding Staramide A28K is an Unreinforced and Heat Stabilized, Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527 |
Eurotec® Tecoform® PO30 GB20 NL HS POM, 20% glass bead reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0334M30L Mica Reinforced |
|||
Tensile Modulus | 3.00 GPa @Temperature -40.0 °C |
435 ksi @Temperature -40.0 °F |
ISO Data |
BASF Ultramid® 8254 HS BK-102 PA6 (Conditioned) Ultramid 8254 HS is a highly flexible, heat stabilized, impact modified nylon 6 extrusion grade for tubing applications. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527-1/-2 |
DSM Akulon® S240-C Nylon 66 (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | |
Ineos ABS NOVODUR® P3TF ABS, Injection Grade
(discontinued **) Injection molding grade, improved flow.Applications: Automotive industry: e.g. wheel trims, instrument panel components.Information provided by the manufacturer.Novodur is produced by Styrolution (2.. |