Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 27.0 GPa | 3920 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-kon DE008E PC (Europe-Africa-Middle East) LNP* Stat-kon* DE008E is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding.This data was supplied by SA.. |
|||
Tensile Modulus | 27.0 GPa | 3920 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP EC008 PEI (Europe-Africa-Middle East) LNP* THERMOCOMP* EC008 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features include: Electrically Conductive. |
|||
Tensile Modulus | 27.0 GPa @Temperature 100 °C |
3920 ksi @Temperature 212 °F |
Wet; EN2561 |
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 37%/7781 Fiber Information provided by HexCel |