Mechanical Properties Metric English Comments
Tensile Modulus 26.2 GPa

@Temperature 23.9 °C
3800 ksi

@Temperature 75.0 °F
Dry; ASTM D638
Park Electrochemical Nelcote® E-766B Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-766B is a low tack, self adhesive epoxy resin system designed for honeycomb applications. E-766B displays excellent peel properties.Key Features and Benefits:Self adhesive resin system f..
Tensile Modulus 26.2 GPa

@Temperature 23.9 °C
3800 ksi

@Temperature 75.0 °F
0° Direction, Dry; 325°F 2kpsi; ASTM D638
Park Electrochemical Nelcote® F-554 Phenolic Prepreg, Chopped Molding Compound Reinforced
Nelcote® F-554 is a high purity silica filled phenolic resin coated on Commercial or Aerospace grade silica fabric. F-554 is used in the manufacture of intermediate temperature ablative rocket nozz..
Tensile Modulus 26.2 GPa

@Temperature 23.9 °C
3800 ksi

@Temperature 75.0 °F
0° Direction, Dry; ASTM D638 Type 1
Park Electrochemical Nelcote® P-670F Polyester Prepreg, 7781 E-Glass Reinforced
Nelcote® P-670F is a versatile, non-styrenated/low VOC polyester resin. P670F is used in a wide variety of applications including tooling and aircraft structures.Key Features and Benefits:Non-styre..
Tensile Modulus 26.2 GPa
3800 ksi
Prepreg, RT, Dry
Renegade Materials Corporation RM-5003 Cyanate Ester Prepreg 4581 Quartz Fabric
Low dielectric and loss, high performance prepreg. 350°F Cure Developed with consistent handling and superior performance Designed for demanding electrical, radome and antennae applications Del..
Tensile Modulus 26.2 GPa
3800 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Therma-Tech™ SF-6000 TC Polyphenylene Sulfide (PPS)  (discontinued **)
Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm..
Tensile Modulus 26.2 GPa
3800 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Lubricomp OFB32I PPS
LNP LUBRICOMP* OFB32I is a compound based on Polyphenylene Sulfide resin containing Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive.This data was supplied by SA..
Tensile Modulus 26.2 GPa
3800 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP OX97635 PPS
LNP LUBRICOMP* OX97635 is a compound based on Polyphenylene Sulfide resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Wear Resistant.
Tensile Modulus 26.2 GPa
3800 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Thermocomp JX89569 PES
LNP THERMOCOMP* JX89569 is a compound based on Polyethersulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 26.2 GPa
3800 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP LC008EXP PEEK (Europe-Africa-Middle East)
LNP* THERMOCOMP* LC008EXP is a compound based on Polyetheretherketone containing Carbon Fiber. Added features include Electrically Conductive, Easy Molding.
Tensile Modulus 26.2 GPa
3800 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Thermocomp JX89569 PES (Asia Pacific)
LNP* THERMOCOMP* JX89569 is a compound based on Polyethersulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Copyright © lookpolymers.com All Rights Reserved