Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 23.19 GPa | 3363 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Faradex DX07304 PC (Asia Pacific) CF filled grade with EMI shieldingThis data was supplied by SABIC-IP for the Asia Pacific region. |