Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 22.9 GPa | 3320 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP EC005R PEI LNP* THERMOCOMP* EC005R is a compound based on Polyetherimide resin containing 25% Carbon Fiber. Added features include: Mold Release, Electrically Conductive. |
|||
Tensile Modulus | 22.9 GPa | 3320 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RC008ESS PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RC008ESS is a compound based on PA66 resin containing Carbon Fiber. Added features include; Electrically Conductive, Easy Molding, Heat Stabilized. |