Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 20.1 GPa | 2920 ksi | transverse; ISO 527-4/5 |
Bond Laminates TEPEX® dynalite 104-RG600(x)/47% Roving Glass – PP Consolidated Composite Laminate Within the TEPEX® composite laminate, PP is a resin known for its good hardness, stiffness, abrasion resistance and chemical resistance.Typical application environments are within automotive applic.. |