Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.90 GPa | 421 ksi | ISO.527 DIN.53455 |
Omnia Plastica Akulon® POM h Acetal Homopolymer The general features of homopolymer acetalic resin are similar to those of copolymer POM c, except that service temperature (under load) is slightly higher but resistance to hydrolysis and strong al.. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® CX2142ME PC+ABS Cycoloy* resin grade CX2142ME is an injection moldable PC/ABS blend with Br- and Cl-free flame retardant systems. Key features of good flow, good impact, UL-94 V0 rating at 1.2 mm, and improved chem.. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® CX2142ME PC+ABS (Asia Pacific) Cycoloy* resin grade CX2142ME is an injection moldable PC/ABS blend with Br- and Cl-free flame retardant systems. Key features of good flow, good impact, UL-94 V0 rating at 1.2 mm, and improved chem.. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics GELOY FXW751SK ASA+PC (Asia Pacific) Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact Resin |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Dry Blend E7364 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Faradex DS0026 PC (Europe-Africa-Middle East) LNP* Faradex* DS0026 is a compound based on Polycarbonate resin containing Flame Retardant, Stainless Steel Fiber. Added features include: EMI/RFI Shielding, Flame Retardant, Non-Brominated & Non-C.. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | ASTM D638 |
LNP Lubricomp® LL-4040 Polyetheretherketone, PTFE Additive
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | ISO 527-1/-2 |
DSM Akulon® K224-HG2U (Cond.) 10% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM CRS5011R PEI (Asia Pacific) Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM CRS5011R PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. Resin is RoHS compliant. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM DH1004 PEI (Europe-Africa-Middle East) High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. RoHS compliant and UL94 V0 listed. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | ISO 527 |
Styrolution Styrolux S SBC Styrolux S is a new developmental, clear styrene-butadiene copolymer (SBC) designed specifically for blending with Styrolux T in order to enable high performance film extrusion and shrink film appli.. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | ISO 527-2 |
Styron VELVEXâ„¢ 5250 SC Reinforced Elastomer/PP compound Overview: VELVEXâ„¢ 5250 SC Natural is a reinforced elastomer/PP compound which provides a unique property balance of good stiffness, impact and high heat resistance in combination with a nice so.. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL EXNL0357 PPE+PS |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be.. |
|||
Tensile Modulus | 2.90 GPa | 420 ksi | ASTM D638 |
Total PSC 500 Polystyrene Polystyrene 500 is a high melt, easy flow crystal polystyrene for fast cycle injection molding. The high flow characteristics of this material make it easy to fill thin parts. 500 is utilized in pro.. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | ISO R527 |
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix HexPly® ES70 is a structural epoxy resin particularly well adapted to low pressure molding processes. This system is versatile and allows a polymerization from 100°C (212°F) up to 150°C (302°F).. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | ISO 527-1/-2 |
DSM Stanyl® TW371 Nylon 46 (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TSGZ-15 PA666-GF15 Product description: Grilon TSGZ-15 is a heat stabilized, normal viscosity, and impact modified PA66 + PA6 injection molding grade with 15% glass fibers. Grilon TSGZ-15 has the following important p.. |
|||
Tensile Modulus | 2.90 GPa | 420 ksi | ASTM D-638 |
Axiall ProTherm® 4529 CPVC Rigid PVC, Molding Georgia Gulf ProTherm® 4529 CPVC is a pelletized injection molding compound designed for large fittings. Typical applications are in potable water and chemical transfer systems especially where hi.. |
|||
Tensile Modulus | 2.90 GPa | 420 ksi | ASTM D-638 |
Axiall 9175J Clear 38 Rigid PVC, Molding, Clear 38 Georgia Gulf 9175J Clear 38 is used for injection blow molding packages in cosmetic and toiletry applications such as hair dyes and shampoos. It has excellent clarity, flow and stability.Informatio.. |
|||
Tensile Modulus | 2.90 GPa | 420 ksi | ASTM D-638 |
Axiall MD-5009 Rigid PVC, Molding Georgia Gulf MD-5009 is a rigid, fitting-grade PVC compound designed for hot spruce/runner molds, large parts and multi-cavity molds. This compound is characterized by excellent processability, whi.. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | ISO 527 - 1 & - 2 |
Asahi Kasei Tenac® 4012 Homopolymer Acetal Resin Medium viscosity grade, with reduced stiffness and increased elongation through addition of special polymersInformation provided by Asahi Kasei Corporation. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | ISO 527 - 1 & - 2 |
Asahi Kasei Tenac® SH210 Homopolymer Acetal Resin Super high-impact grade; highest molecular weight category.Information provided by Asahi Kasei Corporation. |
|||
Tensile Modulus | 2.90 GPa | 420 ksi | ASTM D638 |
Plaskolite West Optix® CA-68 General Purpose Acrylic Resin Injection Molding and Extrusion Grade. Good heat resistance, medium flow. |
|||
Tensile Modulus | 2.90 GPa | 421 ksi | |
LATI Latigea B01 I6 Bio-Polymer Bio-Polymer (PLA, PHB, ...). Unfilled. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p... |