Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.76 GPa | 400 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Packaging 4195 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.76 - 2.96 GPa | 400 - 429 ksi | ASTM D638 |
Proto3000 Accura® 45HC Plastic Stereolithography (SLA) Prototyping Polymer A high speed material, with excellent thermal and moisture resistance for producing functional prototypes in 3D Systems' SLA 250 systems.Benefits:Fast build speed:Provides build speeds that are sign.. |
|||
Tensile Modulus | 2.76 GPa | 400 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® CY5100 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applications |
|||
Tensile Modulus | 2.76 GPa | 400 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Dry Blend E6755 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.76 GPa | 400 ksi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Fittings 87322 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.76 GPa | 400 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and better .. |
|||
Tensile Modulus | 2.76 GPa | 400 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON 9X02785 PC LNP STAT-KON* 9X02785 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Tensile Modulus | 2.76 GPa | 400 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON 9X04323 PPE+PA66 (Asia Pacific) LNP* Stat-kon* 9X04323 is a compound based on Noryl GTX resin,Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | >= 2.76 GPa | >= 400 ksi | |
Master Bond EP30QF Quartz Filled, Two Component Epoxy System Master Bond Polymer System EP30QF is a quartz filled, two component epoxy for high performance bonding, sealing, coating and casting that is formulated to cure at room temperature or more rapidly at.. |
|||
Tensile Modulus | 2.76 GPa | 400 ksi | |
Loctite® 3873 1 component acrylic High Conductivity Flexible Adhesive Thermally Conductive BondersLoctite® Thermally Conductive Adhesives eliminate the need for mechanical fasteners and clips, while providing the most efficient thermal transfer between transistors or.. |
|||
Tensile Modulus | 2.76 - 2.96 GPa | 400 - 429 ksi | ASTM D638 |
3D Systems Accura® 45HC Plastic for SLA® Systems A high speed material, with excellent thermal and moisture resistance for producing functional prototypes in 3D Systems' SLA 250 systems.ApplicationsHigh temperature testing:Automotive "under-the-ho.. |
|||
Tensile Modulus | 2.76 GPa | 400 ksi | ASTM D-638 |
Axiall 9275J Amber 05 Rigid PVC, Molding, Amber 05 Georgia Gulf 9275J Amber 05 is used for injection blow molded packages in cosmetic and toiletry applications. It is a pre-colored amber compound and all ingredients are FDA approved.Information pro.. |
|||
Tensile Modulus | 2.76 GPa | 400 ksi | ASTM Test |
BASF Ultraform N 2320 U03 UNC Q600 POM Ultraform N2320 U03 UNC Q600 is a rapidly freezing UV stabilized general-purpose injection molding grade. |
|||
Tensile Modulus | 2.76 GPa | 400 ksi | ASTM D638 |
Asahi Kasei Thermylene® P6-20FG-0754 20% Glass, Heat Stabilized Information provided by Asahi Thermofil |
|||
Tensile Modulus | 2.76 GPa @Temperature 120 °C |
400 ksi @Temperature 248 °F |
ISO Data |
BASF Ultramid® SEGM35 H1 BK-126 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid SEGM35 H1 BK-126 is a 40% glass/mineral reinforced injection molding grade. It offers enhanced surface appearance, it also exhibits similar UV weathering characteristics compared to 8267G .. |
|||
Tensile Modulus | 2.76 - 3.10 GPa | 400 - 450 ksi | ASTM D790 |
Alcoa KAMA 1120 Prime AntiFog OPS, Sheet
(discontinued **) CapabilitiesGauge: .005’ to .025” (126 to 635µm)Width: 12” to 62” (305 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coati.. |
|||
Tensile Modulus | 2.76 GPa | 400 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ ATH-05KV/000 Acetal (POM) Homopolymer
(discontinued **) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |