Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.41 GPa | 350 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ PC-000/05T-2S Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ PC-000/15T-S2 NATURAL Polycarbonate (PC) Information provided by PolyOne |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® EHA PC+ABS (Asia Pacific) PC+ABS. Electroplateable. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HP1HF PC (Europe-Africa-Middle East) Very high flow, biocompatible polycarbonate for healthcare applications. EtO sterilizable. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | TM R050-36 |
Resinlab® EP750 Clear Unfilled Epoxy Structural Adhesive Resinlab™ EP750 Clear is a two part unfilled epoxy structural adhesive which ingredients are listed in the Code of Federal Regulations Title 21 175.105 (Adhesives) and 175.300 (Resinous and polymer.. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ PF-000/15T Polysulfone, PTFE Lubricated
(discontinued **) Description/Features:PTFE LubricatedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D638 |
LG Chemical Lupoy 1201-10 Polycarbonate Resin Description: LUPOY PC 1201-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D638 |
LG Chemical Lupoy 1301V-10 Polycarbonate Resin Description: LUPOY PC 1301V-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D638 |
LG Chemical Lupoy 1302-07 Polycarbonate Resin Description: LUPOY PC 1302-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Tensile Modulus | 2.41 GPa @Temperature 23.0 °C |
350 ksi @Temperature 73.4 °F |
2; ISO 527-2 |
Solvay Specialty Polymers Amodel® ET-1000 HS Polyphthalamide (PPA) (Dry) Amodel® ET-1000 HS is an impact modified, heat stabilized polyphthalamide (PPA) that exhibits exceptional impact strength and toughness. Like all Amodel® PPA resins, ET-1000 HS offers high fat.. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D638 |
Star Plastics PC741 Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ 201-6 Polycarbonate Resin Overview: CALIBREâ„¢ 201-6 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistance.. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ 301-6 Polycarbonate Resin Overview: CALIBREâ„¢ 300-6 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet applic.. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 4310-10 Polycarbonate EMERGEâ„¢ PC 4310-10 advanced resin is high-performance polycarbonate resin offering high heat resistance and maximum toughness. Applications: Consumer Electronics and Information Technology Eq.. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 4330-15 Polycarbonate EMERGEâ„¢ PC 4330-15 advanced resin is a polycarbonate resin offering ultraviolet light stability, high heat resistance and maximum toughness. Applications: Consumer Electronics and Information.. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ 303V-6 Polycarbonate Resin Overview: CALIBREâ„¢ 303V-6 Polycarbonate resins offer exceptional impact resistance and heat distortion resistance, and meets UL94 V-2 rating. CALIBRE 303V-6 contains a mold release agent, a UV .. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 4330-6 Polycarbonate EMERGEâ„¢ PC 4330-6 advanced resin is a polycarbonate resin offering ultraviolet light stability, high heat resistance and maximum toughness. Applications: Consumer Electronics and Information .. |
|||
Tensile Modulus | >= 2.41 GPa @Temperature 23.9 °C |
>= 350 ksi @Temperature 75.0 °F |
|
Master Bond EP30-3LO Highly versatile, two part epoxy system for bonding, coating, sealing and casting Master Bond EP30-3LO is a two component epoxy system featuring a combination of optical clarity and light transmission, good glass transition temperature (Tg), great chemical resistance along with p.. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D638 |
Ensinger Tecamid® HS Nylon (PA) Heat Stabilized nylon, increased ability to withstand the negative effects of heat exposure and increased overall service temperature over nylon 6/6.Information provided by Ensinger, Inc. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | ASTM D-638 |
Axiall HHW-191 Rigid PVC, Extrusion Georgia Gulf HHW-191 is a special purpose profile extrusion alloy designed for applications requiring the following properties: Excellent WeatherabilityImpact Strength & ToughnessColorabilityChemic.. |
|||
Tensile Modulus | 2.41 GPa | 350 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ MP-20CF/15T Modified Polyphenylene Oxide (mPPO), Carbon Fiber Reinforced, PTFE Lubricated
  Description/Features:Carbon Fiber ReinforcedPTFE LubricatedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |