Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.32 GPa | 336 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Packaging 161JA White Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.32 GPa | 336 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Packaging 2020 LO-TB Polyvinyl Chloride, Rigid (PVC, Rigid) Geon® 2020 LO-TB is a clear blue tint pellet compound designed for water bottle and other low odor appliations that require FDA sanctioned materials.Information provided by PolyOne |
|||
Tensile Modulus | 2.32 GPa | 336 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Packaging 2798 Polyvinyl Chloride, Rigid (PVC, Rigid) Premium chemical resistant Compound for Packaging.Information provided by PolyOne |
|||
Tensile Modulus | 2.32 GPa | 336 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 123X PC Copolymer Improved flow PC with excellent processability and mold release. |
|||
Tensile Modulus | 2.32 GPa | 336 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® 123X PC Copolymer (Europe-Africa-Middle East) Improved flow PC with excellent processability and mold release.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 2.32 GPa | 336 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXD1433T PC Copolymer Clear PC-siloxane copolymer with excellent processability in special light diffusion colors. Medium flow, UV stabilized. Improved toughness compared to standard PC in same color. Color package may .. |
|||
Tensile Modulus | 2.32 GPa | 336 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXD1433T PC Copolymer (Asia Pacific) Clear PC-siloxane copolymer with excellent processability in special light diffusion colors. Medium flow, UV stabilized. Improved toughness compared to standard PC in same color. Color package may .. |
|||
Tensile Modulus | 2.32 GPa | 336 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXD1433T PC Copolymer (Europe-Africa-Middle East) Clear PC-siloxane copolymer with excellent processability in special light diffusion colors. Medium flow, UV stabilized. Improved toughness compared to standard PC in same color. Color package may .. |
|||
Tensile Modulus | 2.32 GPa | 336 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXM1413T PC Copolymer PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Tensile Modulus | 2.32 GPa | 336 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXM1413T PC Copolymer (Asia Pacific) PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Tensile Modulus | 2.32 GPa | 336 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXM1413T PC Copolymer (Europe-Africa-Middle East) PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supplied by .. |
|||
Tensile Modulus | 2.32 GPa | 336 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 143X PC Copolymer (Asia Pacific) Improved flow PC with excellent processability and mold release. |
|||
Tensile Modulus | 2.32 GPa | 336 ksi | ASTM D638 |
Spartech Solarex® SV Copolyester Sheet Description: Copolyester SheetInformation provided by Spartech. |
|||
Tensile Modulus | 2.32 GPa | 336 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP DX11354X PC (Asia Pacific) LNP* Thermocomp* Compound DX11354X is a colorable PC based compound with stable plating and RF performance, colored LDS material solution, good surface and processing window, high impact strength. I.. |
|||
Tensile Modulus | 2.32 GPa | 336 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-kon DS0029 PC LNP STAT-KON* DS0029 is a compound based on Polycarbonate resin containing Stainless Steel. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for t.. |
|||
Tensile Modulus | 2.32 GPa | 337 ksi | ASTM D-638 |
Axiall Suprel® SVA 9812 Rigid PVC, Extrusion Georgia Gulf Suprel® SVA 9812 Alloy is an extrusion grade thermoplastic designed for sheet or profile applications requiring high impact resistance. Key features of Suprel 9812 alloy are flame ret.. |
|||
Tensile Modulus | 2.32 GPa | 336 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 123X PC Copolymer (Asia Pacific) Improved flow PC with excellent processability and mold release. |
|||
Tensile Modulus | 2.32 GPa @Temperature 120 °C |
336 ksi @Temperature 248 °F |
ISO Data |
BASF Ultramid® SEGM35 H1 BK-126 15/25% Glass/Mineral Filled PA6 (Conditioned) Ultramid SEGM35 H1 BK-126 is a 40% glass/mineral reinforced injection molding grade. It offers enhanced surface appearance, it also exhibits similar UV weathering characteristics compared to 8267G .. |