Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.20 GPa | 319 ksi | |
Plastcom SLOVALEN PC 71 T 10 PP, 10% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 10% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decr eased shri.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Cycolac® X15 ABS Automotive. Very high heat resistance with high impact. UL94 HB rated. High gloss.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® XCY620 PC+ABS (Europe-Africa-Middle East) PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Eur.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | ISO 527-1/-2 |
Quadrant EPP Symalit® 1000 PVDF unfilled, extruded (ISO Data) Symalit 1000 PVDF is a highly crystalline unreinforced fluoropolymer combining good mechanical, thermal and electrical properties with excellent chemical resistance. It also shows good resistance to.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® CFR9712 PC COPOLYMER Lexan* CFR9712 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 2.0 mm and high flow capability. .. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DL002 PC (Europe-Africa-Middle East) LNP* Lubricomp* DL002 is a compound based on Polycarbonate resin containing PTFE. Added features include: Internally Lubricated. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | |
Polycasa Acryl® KR 2015/1 Acrylic, Impact Grade Medium-impact grade with very good flow behavior, especially mechanically stressed parts with long flow paths; e.g. strip light diffusers. Can be extruded into thin tubes, sheet and film.Data was c.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | 1 mm/min |
Polimeri Europa EDISTIR RK0414 High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,088-03-04-23 UL94 V-0, polybromobiphenylether (PBBE) free, flame retarded high impact polystyrene with excellent light .. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXD9810U PC Copolymer (Asia Pacific) Polycarbonate with high flow, excellent processability, good impact and thermal properties, UV stabilized, non-Chlorine and non-Bromine flame retardant, UL rated V-0 and V-1. Available in limited di.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | |
Ineos ABS Lustran® 723-1, Extrusion Grade
(discontinued **) Extrusion grade for refrigerator inliner.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | ASTM D638 |
Covestro Apec® DP9-9331 High-Heat Polycarbonate, General Purpose
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Tensile Modulus | 2.20 GPa @Thickness 3.20 mm |
319 ksi @Thickness 0.126 in |
1mm/min; ASTM D638 |
LG Chemical LI970HF Co-Extrusion ASA Description: Good Weatherability, Scratch Resistance, High FlowApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | |
LATI Latilub 87/28-20T PC, PTFE Filled Self-lubricating product based on Polycarbonate (PC). PTFE.Information provided by Lati Industria Termoplastici S.p.A. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | |
LATI Latistat 63-08 PA6, Impact Modified Dissipative product based on Polyamide 6 (PA6), impact modified. Unfilled.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DX96651 PC (Asia Pacific) LNP LUBRICOMP* DX96651 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® CL100 PBT+PC Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GTX GTX963 PPE+PA (Europe-Africa-Middle East) NORYL GTX963 is an unfilled impact modified material with excellent heat properties and good processability. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX973 PPE+PA (Europe-Africa-Middle East) NORYL GTX973 is a material especially designed for electrostatic painting and powder coating applications. The material combines high heat resistance with impact and conductivity in a unique way. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL N110 PPE+HIPS (Europe-Africa-Middle East) NORYL N110 is an unfilled material, with a Vicat B/120 of 115 °C according ISO 306. NORYL N110 has medium temperature resistance and good |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | ASTM-D790 |
Polyram RamTal PM1409 Acetal, PTFE Filled Polyacetal filled with PTFE for sliding parts, low friction and improved wear resistance in molded parts.Information provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | ASTM D882 |
Eastman Eastobond 19412 Copolyester, Film Eastobond 19412 is a terephthalate-based copolyester. It is identical to our 19411 resin in every aspect, except that the 19412 has been crystallized for drying purposes and ease of handling. Eastob.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | ISO 527-1/-2 |
Covestro Makroblend® DP UT6003 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendimpact modifiedUV-stabilizedinjection molding grade Makroblend DP UT6003* offers an exceptional low-temperature impact strength, good flowability and excellent c.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | ISO 527-1/-2 |
Covestro Makroblend® DP UT6005 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendimpact modifiedeasy releaseinjection molding grade Makroblend DP UT6005* offers an exceptional low-temperature impact strength, good flowability and excellent ch.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 3959 black 9992 PA610 Product description: Grilamid XE 3959 is a high viscosity Polyamide 610 especially suitable for extrusion applications. This PA610 product is to a large extent based on renewable raw materials and i.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | ASTM D638 |
Aclo Accutech Polypropylene CP0435G20CV Copolymer Glass Reinforced Coupled Approved to GMP.PP.029 |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0339C40L1 Calcium Reinforced |
|||
Tensile Modulus | 2.20 - 3.50 GPa | 319 - 508 ksi | ASTM D638 |
Adamas Rixon U PEEK, Unreinforced Information provided by Adamas, HPM |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | ISO 527-1/-2 |
Covestro Makroblend® DP UT6007 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendimpact modifiedeasy releaseUV-stabilizedinjection molding grade Makroblend DP UT6007* offers an exceptional low-temperature impact strength, good flowability and.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL RN0611 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0611 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | ISO 527-1, -2; 1 mm/min |
Lanxess Pocan® C 1206 000000 PET + PC PET + PC, non-reinforced, injection molding, improved impact strengthInformation provided by LANXESS. |