Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.14 GPa | 310 ksi | ASTM D638 |
Ineos Nova FX550 (ASTM) Advanced Styrenic Polymer
(discontinued **) Extremely high glossHigh Izod impact strengthUL Classification 94 HBPractical toughnessHigh flow for injection moldingScuff resistanceApplications: Replacement resin for selected ABS applicationsRef.. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | ASTM D638 |
Ineos Nova Zylar® 390 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features: Excellent clarityHigh flexural modulusGood toughness and elongationStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationMeets USP XXIII specification.. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp DP0039 PC LNP* Lubricomp* DP0039 is a Polycarbonate base resin containing PTFE and Silicone lubricants. Characteristics are: Flame Retardant.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp FFL21 PE LNP* Lubricomp* FFL21 is a compound based on Polyethylene resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for t.. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp ML002S PP LNP* Lubricomp* ML002S is a compound based on Polypropylene containing PTFE. Characteristics of this grade are: Heat Stabilized and Internally Lubricated.This data was supplied by SABIC-IP for the.. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRILOY D2000 PC (Asia Pacific) LNP LUBRILOY* D2000 is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | ASTM D638 |
Spartech CamAlloy /ABS Weatherable Sheet Description: Weatherable SheetInformation provided by Spartech. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | ASTM D638 |
Spartech Korad® SP-9011 Cap ABS Sheet Description: ABS SheetInformation provided by Spartech. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | ASTM D638 |
Spartech Korad® SP-9071 FR/ABS Flame Retardant Sheet Description: Flame Retardant SheetKorad is a registered trademark of Polymer Extruded Products, Inc..Information provided by Spartech. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | ASTM D638 |
Spartech SP-9010 General Purpose ABS Sheet Description: ABS SheetInformation provided by Spartech. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | ASTM D638 |
Spartech SP-9020 Premium ABS Sheet Description: ABS SheetInformation provided by Spartech. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | ASTM D638 |
Spartech SP-9070 ABS/PVC Flame Retardant Sheet Description: Flame Retardant SheetInformation provided by Spartech. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON WS002I PBT LNP* STAT-KON* WS002I is a compound based on PBT resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, High Impact. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics XYLEX HX7509HP PC+POLYESTER Medium flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), fo.. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics XYLEX X7509HP PC+POLYESTER (Asia Pacific) PC+Polyester alloy. Houseware applications. USA/Europe Food contact. this grade will no longer be supported with biocompatibility information and should not be used for medical applications which r.. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | ASTM D 638 |
Styrolution Zylar 650 MBS Zylar® 650 is an impact modified styrene acrylic copolymer that provides a balance of clarity and toughness, with outstanding strength and rigidity. Zylar 650 also has superior processing charact.. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® MP-0670 ABS, Metal Plating Grade Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl HIPS3191 PS This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Xylex X7529 PC+POLYESTER (Asia Pacific) PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical quality. UV 400nm block.This data was supplied by SABIC-IP for the Asia Pacif.. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Xylex X7529 PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical quality. UV 400nm block.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Xylex X7529OQ PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical qualityThis data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | ASTM D638 |
Westlake Plastics Absylux® Acrylonitrile-Butadiene-Styrene, Compression Molded Compression molded Absylux ABS is a low cost engineering plastic ideal for prototyping. It has excellent dimensional stability and lends itself to all forms of fabricationInformation provided by We.. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | ASTM D638 |
Total PSI 825EX Polystyrene Polystyrene 825EX is a high impact polystyrene designed for high stiffness in extrusion/thermoforming applications. The balance of high stiffness and impact properties allow for light weighting of t.. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | ASTM D638 |
Ineos Nova Zylar® 631 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features:Outstanding practical toughness and ductilityStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationUSP Class VI compliantCustom colors and enhancement .. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Xylex X7529OQ PC+POLYESTER (Asia Pacific) PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical qualityThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 2.14 GPa | 310 ksi | |
Ineos ABS Centrex® HGM ASA Blend
(discontinued **) Key Features:UnfilledLight stabilized or stable to lightU.V. stabilized or stable to weatherHeat stabilized or stable to heatSuitable processing methods:Injection moldingInformation provided by Baye.. |