Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.12 GPa | 307 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® EXL1036 PC Copolymer Lexan* EXL1036 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high viscosity grade designed for (co-)extrusion. This resin offers extreme low temperature (-60 C) ductility and good h.. |
|||
Tensile Modulus | 2.12 GPa | 307 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL1036 PC Copolymer (Asia Pacific) Lexan* EXL1036 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high viscosity grade designed for (co-)extrusion. This resin offers extreme low temperature (-60 C) ductility and good h.. |
|||
Tensile Modulus | 2.12 GPa | 307 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® EXL1036 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1036 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high viscosity grade designed for (co-)extrusion. This resin offers extreme low temperature (-60 C) ductility and good h.. |
|||
Tensile Modulus | 2.12 GPa | 307 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer 11 MFR LEXAN High Flow Ductile Copolymer |
|||
Tensile Modulus | 2.12 GPa | 307 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer (Asia Pacific) 11 MFR LEXAN High Flow Ductile Copolymer |
|||
Tensile Modulus | 2.12 GPa | 307 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP AI001XXH ABS LNP* Lubricomp* AI001XXH is a compound based on ABS containing 2% Silicone. Characteristics of this grade are: Healthcare and Internally Lubricated. |
|||
Tensile Modulus | 2.12 GPa | 307 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXRL0683 PC Copolymer 11 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.12 GPa | 307 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer (Europe-Africa-Middle East) 11 MFR LEXAN High Flow Ductile Copolymer |
|||
Tensile Modulus | 2.12 GPa | 307 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer 11 MFR LEXAN High Flow Ductile Copolymer UV stabilized, available in transparent colors only |
|||
Tensile Modulus | 2.12 GPa | 307 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer (Asia Pacific) 11 MFR LEXAN High Flow Ductile Copolymer UV stabilized |
|||
Tensile Modulus | 2.12 GPa | 307 ksi | ISO 527-2 |
Kureha KF Polymer 2950 PVDF Copolymer KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p.. |
|||
Tensile Modulus | 2.12 GPa | 307 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DP0039EF PC (Asia Pacific) LNP* Lubricomp* DP0039EF is a compound based on Polycarbonate resin containing Silicone, PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.12 GPa | 307 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRILOY D20001 PPO LNP* LUBRILOY* Z20001 is a compound based on PPO resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, Flame Retardant. |
|||
Tensile Modulus | 2.12 GPa | 307 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON CD0001 PS LNP* STAT-KON* CD000I is a compound based on Polystyrene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Tensile Modulus | 2.12 GPa | 307 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON CD000I PS LNP* Stat-kon* CD000I is a compound based on Polystyrene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Tensile Modulus | 2.12 GPa | 307 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP 67002XXH PBT+PC LNP* THERMOCOMP* 67002XXH is a compound based on PBT+PC containing proprietary antimicrobial additives. Designed for touch surfaces in patient critical healthcare applications. Added features inc.. |
|||
Tensile Modulus | 2.12 GPa | 307 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP 9X04488 POLYPHENYLENESULFONE (Asia Pacific) LNP* Thermocomp* 9X04488 is a compound based on POLYPHENYLENESULFONE resin containing Mineral. |
|||
Tensile Modulus | 2.12 GPa | 307 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP 9X04488 PPS LNP* THERMOCOMP* 9X04488 is a compound based on PPS resin containing Mineral. |
|||
Tensile Modulus | 2.12 GPa | 307 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PKN4775 PPE+PS PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack.. |
|||
Tensile Modulus | 2.12 GPa | 307 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL PKN4775 PPE+PS PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack.. |
|||
Tensile Modulus | 2.12 GPa | 307 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PKN4775 PPE+PS (Asia Pacific) PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack.. |
|||
Tensile Modulus | 2.12 GPa | 307 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL PKN4775 PPE+PS (Asia Pacific) PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack.. |
|||
Tensile Modulus | 2.12 GPa | 307 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PKN4775 PPE+PS (Europe-Africa-Middle East) PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack.. |
|||
Tensile Modulus | 2.12 GPa | 307 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL PKN4775 PPE+PS (Europe-Africa-Middle East) PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack.. |
|||
Tensile Modulus | 2.12 GPa | 307 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON RD000I PA 66 LNP* STAT-KON* RD000I is a compound based on Nylon 66 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Tensile Modulus | 2.12 GPa | 307 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp 9X04488 POLYPHENYLENESULFONE LNP* Thermocomp* 9X04488 is a compound based on POLYPHENYLENESULFONE resin containing Mineral.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.12 GPa | 307 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer (Europe-Africa-Middle East) 11 MFR LEXAN High Flow Ductile Copolymer UV stabilized, available in transparent colors only |
|||
Tensile Modulus | 2.12 GPa | 307 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRILOY Z20001 PPO LNP* Lubriloy* Z20001 is a compound based on PPE+PS Blend resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, Flame Retardant. |