Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® MC8100 PC+ABS (Asia Pacific) Extrusion blowmolding grade. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FXG1414T PC Copolymer PC-siloxane copolymer in special ""Diamond Sparkle"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Colorcomp D10009 PC LNP* Colorcomp* D10009 is a compound based on Polycarbonate resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant.This data was supplied .. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Colorcomp D10009 PC (Asia Pacific) LNP* Colorcomp* D10009 is a compound based on Polycarbonate resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant.This data was supplied .. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DL001 PC LNP* LUBRICOMP* DL001 is a compound based on Polycarbonate resin containing 5% PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DL001 PC (Asia Pacific) LNP* Lubricomp* DL001 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DL002ER PC LNP* Lubricomp* DL002ER is a compound based on Polycarbonate resin containing 10% PTFE. Added features of this material include: Internally Lubricated, Easy Molding, Mold Release. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DL003 PC LNP LUBRICOMP* DL003 is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DL003 PC (Asia Pacific) LNP LUBRICOMP* DL003 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.06 GPa @Thickness 3.20 mm |
299 ksi @Thickness 0.126 in |
1 mm/min; ASTM D638 |
LG Chemical TR300 MABS, Flame Retardant, Transparency Feature: Injection Molding, Flame Retardant, TransparencyApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9010-94-0 and 25713-60-4Information provided by LG Ch.. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DL0049EF PC (Asia Pacific) LNP* Lubricomp* DL0049EF is a compound based on Polycarbonate resin containing PTFE, Flame Retardant. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DX98306H PC LNP* LUBRICOMP* DX98306H is a compound based on Polycarbonate resin containing Proprietary Fillers. Added features of this material include: Wear Resistant, Low Extractible. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp GL004 PSU (Asia Pacific) LNP* Lubricomp* GL004 is a compound based on Polysulfone resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pacifi.. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP IL004 PA 6/12 LNP* LUBRICOMP* IL004 is a compound based on Nylon 6/12 resin containing 20% PTFE. Added features of this material include: Wear Resistant. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP IL004 PA 6/12 (Asia Pacific) LNP* Lubricomp* IL004 is a compound based on Nylon 6/12 resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP KP004L Acetal Copoly LNP* LUBRICOMP* KP004L is a compound based on Acetal Copolymer resin containing 20% PTFE/Silicone. Added features of this material include: Wear Resistant, Low Extractible. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp QP003 PA 6/10 LNP* Lubricomp* QP003 is a compound based on Nylon 6/10 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Am.. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp QP003 PA 6/10 (Asia Pacific) LNP* Lubricomp* QP003 is a compound based on Nylon 6/10 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the As.. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP ZL003 PPE+PS LNP* LUBRICOMP* ZL003 is a compound based on PPE+PS resin containing 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRILOY D20009P PC (Asia Pacific) LNP* Lubriloy* D20009P is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Internally Lubricated, Flame Retardant,.. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRILOY K2000 Acetal LNP LUBRILOY* K2000 is a compound based on Acetal resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRILOY K2000 Acetal (Asia Pacific) LNP LUBRILOY* K2000 is a compound based on Acetal resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY A3000 ABS LNP STAT-LOY* A3000 is a compound based on ABS resin. Added feature of this material is: Antistatic. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY A3000 ABS (Asia Pacific) LNP STAT-LOY A3000 is a compound based on Acrylonitrile butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistatic. Also known as: STAT-LOY A |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® HI-1001BN PC/ABS, Unreinforced PC/ABS that is used for the housing of mobile phone, wheel cap, rice cooker, electric iron etc., refrigerator door handle, panel etc.Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® SF-0505HWR MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® SF-0505HWR MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl MX5569 PPE+PS PPE+PS blend. High Heat. Good balance of flow and impact. Offers good aging performance under heat. Typical applications include Automotive Interiors and Lighting.This data was supplied by SABIC-.. |
|||
Tensile Modulus | 2.06 GPa @Temperature -70.0 °C |
299 ksi @Temperature -94.0 °F |
DAM; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 330 NC010 Nylon
(Unverified Data**) Unreinforced PolyamideZytel 330 NC010 is a transparent polyamide resin with amorphous characteristics.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DL002ER PC (Asia Pacific) LNP* Lubricomp* DL002ER is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated, Easy Molding, Mold Release. |