Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.003 GPa @Temperature 23.0 °C |
290.5 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® ST800HSL BK152 Nylon 66
(Unverified Data**) Zytel® ST800HSL BK152 is a heat stabilized Super Tough black polyamide 66 resin. It offers outstanding impact resistance, high productivity and laser markability.Information provided by DuPont |
|||
Tensile Modulus | 2.003 GPa | 290.5 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® ST800HSL BK152 Nylon 66
(Unverified Data**) Super Toughened Heat Stabilized Polyamide 66 Zytel ST800HSL BK152 is a heat stabilized Super Tough black polyamide 66 resin. It offers outstanding impact resistance high productivity and laser marka.. |