Polymer Property : Tensile Modulus = 19.98 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 19.98 GPa
2898 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON AX02747 ABS (Asia Pacific)
LNP* Stat-kon* AX02747 is a compound based on Acrylonitrile Butadiene Styrene resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive.