Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 18.0 GPa | 2610 ksi | ISO 527-2 |
PolyOne OnForce™ LFT NN-60LGF/000 HS UV Black Polyamide 66 (Nylon 66) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Tensile Modulus | 18.0 GPa | 2610 ksi | |
PBI Performance Products Celazole® TL-60 Self Lubricating Melt Processable Polybenzimidazole Celazole® polybenzimidazole (PBI) resin is a unique and highly stable linear hetrocyclic polymer. PBI is characterized by high strength; excellent thermal stability, and broad chemical resistance. .. |
|||
Tensile Modulus | 18.0 GPa | 2610 ksi | ISO 527-2 |
Solvay Specialty Polymers Ixef® 2011 Polyarylamide (PARA), 42% Mineral Filler
(discontinued **) Ixef 2011 is a general purpose, 42% mineral reinforcedpolyarylamide which exhibits high strength and stiffness, low warpage, and outstanding surface gloss.- Black: Ixef 2011/9000- Custom ColorableFe.. |
|||
Tensile Modulus | 18.0 GPa | 2610 ksi | ISO 527 Type 1A |
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, Conditioned Description: TECHNYLSTARâ„¢ AFX 218 V60 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 60% of glass fiber, for injection molding.Benefits: Due.. |
|||
Tensile Modulus | 18.0 GPa | 2610 ksi | ISO 527-1 |
Vyncolit Neopreg Kinel® SK61 L5G Glass Fiber Reinforced Molding Compound Epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particular suited for over molding.. |
|||
Tensile Modulus | 18.0 GPa | 2610 ksi | ISO 527-1 |
Vyncolit TX10916/15 Graphite Filled Novolac Phenolic Novolac resin based, graphite filled compound used for low friction applications where dimensional stability is requiredInformation provided by Sumitomo Bak North America, Inc. |
|||
Tensile Modulus | 18.0 GPa | 2610 ksi | ISO 527-1 |
Vyncolit A2990 Glass Fiber Reinforced Novolac Phenolic Resole resin based, glass fiber reinforced. Good mechanical properties, combined with superior electrical insulation properties. Among others used for commutator applicationsInformation provided by .. |
|||
Tensile Modulus | 18.0 GPa | 2610 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-5 FWA black 9225 PA*-GF50 Product description: Grivory GV-5 FWA black 9225 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copoly.. |
|||
Tensile Modulus | 18.0 GPa | 2610 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-5H black PA*-GF50 Product description: Grivory GV-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Tensile Modulus | 18.0 GPa | 2610 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-5H EF nat PA*-GF50 Product description: Grivory GV-5H EF natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyam.. |
|||
Tensile Modulus | 18.0 GPa | 2610 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-5H PA*-GF50 Product description: Grivory GV-5H natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyamide.. |
|||
Tensile Modulus | 18.0 GPa | 2610 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® LV-65H FWA black 9225 PA12-GF65 Product description: Grilamid LV-65H FWA black 9225 is a 65 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combine.. |
|||
Tensile Modulus | 18.0 GPa | 2610 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® LV-65H FWA nat PA12-GF65 Product description: Grilamid LV-65H FWA natural is a 65 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w.. |
|||
Tensile Modulus | 18.0 GPa | 2610 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® LV-65H SST black 9288 PA12-GF65 Product description: Grilamid LV-65H SST black 9288 is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12, designed for complex structural parts with the f.. |
|||
Tensile Modulus | 18.0 GPa | 2610 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® LV-65H SST nat PA12-GF65 Product description: Grilamid LV-65H SST natural is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12, designed for complex structural parts with the foll.. |
|||
Tensile Modulus | 18.0 GPa | 2610 ksi | ISO 527 |
Eurotec® Tecodur® PB70 GR50 NL100 PBT, 50% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Tensile Modulus | 18.0 GPa | 2610 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® HT1V-5 FWA black 9225 PA6T/6I-GF50 Product description: Grivory HT1V-5 FWA black 9225 is a 50 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: .. |
|||
Tensile Modulus | 18.0 GPa | 2610 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® HT1V-5 FWA nat PA6T/6I-GF50 Product description: Grivory HT1V-5 FWA natural is a 50 wt.-% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6.. |
|||
Tensile Modulus | 18.0 GPa | 2610 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® HT1V-5 HY black 9205 PA6T/6I-GF50 Product description: Grivory HT1V-5 HY black 9205 is a 50% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-5 HY bl.. |
|||
Tensile Modulus | 18.0 GPa | 2610 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-5 FWA nat PA*-GF50 Product description: Grivory GV-5 FWA natural is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Tensile Modulus | 18.0 GPa | 2610 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GVX-5 H black 9915 PA*-GF50 Product description: Grivory GVX-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam.. |
|||
Tensile Modulus | 18.0 GPa | 2610 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GVX-5 H nat PA*-GF50 Product description: Grivory GVX-5H natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamid.. |
|||
Tensile Modulus | 18.0 GPa | 2610 ksi | ASTM D638 |
Solvay Specialty Polymers Ixef® 2530/X9027 Polyarylamide, 55% Mineral + Glass Fiber, at Equilibrium (65% RH)
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Tensile Modulus | 18.0 GPa | 2610 ksi | ISO 527 |
Polyram Polytron A50B01 Nylon 6.6, 50% Long Fiber Glass 50% Long fiber glass reinforced black Nylon 6.6, heat stabilized for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 18.0 GPa | 2610 ksi | ISO 527-1/-2 |
DSM Stanyl® 46HF5050 Nylon 46-50% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Tensile Modulus | 18.0 GPa | 2610 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® AF-1145 V0 Polyphthalamide (PPA) Resin, 45% Glass Reinforced, at 50% RH
(di AMODEL AF-1145 V0 is a 45% glass reinforced, flame retarded polyphthalamide (PPA) which exhibits a high heat distortion temperature, high tensile strength and flexural modulus. The material is rela.. |