Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 16.44 GPa | 2384 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp 5C004 LNP* Thermocomp* 5C004 is a compound based on Polyvinylidene Fluoride resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC.. |
|||
Tensile Modulus | 16.44 GPa | 2384 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP 5C004 FP-V (PVDF) LNP* THERMOCOMP* 5C004 is a compound based on Polyvinylidene Fluoride resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 16.44 GPa | 2384 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP 5C004 PVDF (Asia Pacific) LNP* Thermocomp* 5C004 is a compound based on Polyvinylidene Fluoride resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |