Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 13.85 GPa | 2009 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP RF0069SZ PA 66 (Asia Pacific) LNP* Thermocomp* RF0069SZ is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant. |
|||
Tensile Modulus | 13.85 GPa | 2009 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP VERTON RV008S PA 66 LNP* VERTON* RV008S is a compound based on Nylon 66 resin containing 40% Long Glass Fiber. Added features of this material include: Heat Stabilized, Structural. |
|||
Tensile Modulus | 13.85 GPa | 2009 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP VERTON RV008S PA 66 (Asia Pacific) LNP* Verton* RV008S is a compound based on Nylon 66 resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized. |