Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 13.2 GPa | 1910 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID 6 GF 40 Polyamide 6, 40% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 40% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Tensile Modulus | 13.2 GPa | 1910 ksi | ASTM D638 |
Premix Premi-Glas® 3101-22 Fiberglass Reinforced Thermoset BMC Premi-Glas® 3101-22 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.Key features and .. |
|||
Tensile Modulus | 13.2 GPa @Temperature 23.0 °C |
1910 ksi @Temperature 73.4 °F |
ISO 527 |
PolyOne Bergamid™ PA66 C20 Black Polyamide 66 (Nylon 66) Product code EM00000364BIInformation provided by PolyOne |
|||
Tensile Modulus | 13.2 GPa | 1910 ksi | ASTM D638 |
Plenco 51240 PET, Pellet, Injection Molded, Blue
(discontinued **) PLENCO 51240 is an engineering grade glass reinforced flame retarded recycled polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed.Information supplied by P.. |
|||
Tensile Modulus | 13.2 GPa | 1910 ksi | ASTM D638 |
LNP Thermocomp® LF-1006 Polyetheretherketone, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Tensile Modulus | 13.2 GPa | 1910 ksi | ASTM D638 |
Plenco 08218 Polyester BMC, Compression Molded PLENCO 08218 is a renumber of PlasGlas 20118. PLENCO 08218 is an 18% glass-filled polyester bulk molding compound characterized as an electrical grade, but has many outstanding properties that make .. |
|||
Tensile Modulus | 13.2 GPa | 1910 ksi | ASTM D638 |
Plenco 1508 Polyester, Briquette, Transfer Molded PLENCO 01508 is a mineral filled pelletized polyester molding compound, which offers excellent heat resistance and electrical properties. UL recognized under component file E40654. 01508 is availabl.. |
|||
Tensile Modulus | 13.2 GPa | 1910 ksi | ASTM D638 |
Plenco 5118 Phenolic, Granular, Injection Molded PLENCO 05118 is a mineral and graphite filled phenolic molding compound, formulated for bearing seals. 05118 provides for a low coefficient of friction, abrasion resistance, minimal water absorptio.. |