Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 13.1 GPa | 1900 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP KONDUIT RTF2B PA 66 (Europe-Africa-Middle East) LNP* Konduit* RTF2B is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Tensile Modulus | 13.1 GPa | 1900 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance.. |
|||
Tensile Modulus | 13.1 GPa | 1900 ksi | Conditioned; ASTM D638 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance.. |
|||
Tensile Modulus | 13.1 GPa | 1900 ksi | Conditioned; ASTM D638 |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0.. |
|||
Tensile Modulus | 13.1 GPa | 1900 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0.. |
|||
Tensile Modulus | 13.1 GPa | 1900 ksi | ASTM D638 |
PolyOne Edgetek® LCP-15GF/000 Liquid Crystal Polymer - 15% Fiber Glass
(discontinued **) Data provided by PolyOne. |
|||
Tensile Modulus | 13.1 GPa | 1900 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® SF-30GF/000 Polyphenylene Sulfide (PPS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 13.1 GPa | 1900 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater th.. |
|||
Tensile Modulus | 13.1 GPa | 1900 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater th.. |
|||
Tensile Modulus | 13.1 GPa | 1900 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP LF006 PEEK (Asia Pacific) LNP* Thermocomp* LF006 is a compound based on Polyetheretherketone resin containing Glass Fiber. |
|||
Tensile Modulus | 13.1 GPa | 1900 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP UF006H PPA LNP* THERMOCOMP* UF006H is a compound based on Polyphthalamide resin containing 30% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Tensile Modulus | 13.1 GPa | 1900 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist.. |
|||
Tensile Modulus | 13.1 GPa | 1900 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOTUF PF008IR PA 6 LNP* Thermotuf* PF008IR is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: High Impact, Mold Release. |
|||
Tensile Modulus | 13.1 GPa | 1900 ksi | ASTM D638 |
Applied Composites 8007 Polyester SMC Industry Application: ConstructionProduct Application: Water TreatmentDistinct Features: Pigmentable, Low Water Absorption, Weathering Resistant, Good Corrosion Resistance in Waste Water Environment.. |
|||
Tensile Modulus | 13.1 GPa | 1900 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® A3 GF 40 (1258) PA 6.6 Dry, 40% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Tensile Modulus | 13.1 GPa | 1900 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOTUF PF008IR PA 6 (Asia Pacific) LNP* Thermotuf* PF008IR is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: High Impact, Mold Release. |
|||
Tensile Modulus | 13.1 GPa | 1900 ksi | ASTM D638 |
LNP Lubricomp® PDX-O-88533 BK8-229 Polyphenylene Sulfide, Glass Fiber Reinforcement, PTFE Lubricant
(disconti Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |