Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 12.5 GPa | 1810 ksi | |
Plastcom SLOVAMID 6 GF 35 FRC 5 PA6 reinforced with 35% glass fibre, with flame retardant PA 6 for injection moulding, chemically reinforced with 35 % glass fibre, with halogen free flame retardant. Main features: flammability in accordance with UL 94 V2 at 1.6 mm, glow wire at 750°C, C.. |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | same value from ASTM and ISO test. |
BASF Capron® GR40 HS 40% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron GR40 HS is a heat stabilized 40% glass reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensional stabil.. |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | ISO 527-2 |
PolyOne Edgetek® AM-35GF/000 FR NH Polyphthalamide (PPA) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | cond.; ISO 527-1, -2; 1 mm/min |
Lanxess Durethan® DP BKV 60 EF 000000 Nylon6, 60% Glass Fiber PA 6, 60% glass fibers, injection molding, improved flowabilityInformation provided by LANXESS. |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218 V50 PA66, 50% glass fiber, Conditioned Description: TECHNYL® A 218 V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | ISO 527 Type 1A |
Solvay TECHNYLSTARâ„¢ AFX 218 V50 PA6, 50% glass filled, Conditioned Description TECHNYLSTARâ„¢ AFX 218 V50 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. It is availab.. |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® AS-1935 HS Polyphthalamide (PPA), 35% Glass Fiber Amodel® AS-1935 HS is a 35% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e.. |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-kon AE004E ABS LNP* Stat-Kon* AE004E is an ABS compound containing Glass Fiber. Characteristics of this grade are Statically Conductive and Easy Molding.This data was supplied by SABIC-IP for the Americas region... |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP DF0081PI PC (Asia Pacific) LNP* Thermocomp* DF0081PI is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High Modulus, good flatness, Non-Brominated & .. |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOTUF RF008IS PA 66 LNP* Thermotuf* RF008IS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOTUF RF008IS PA 66 (Asia Pacific) LNP* Thermotuf* RF008IS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON RX03013 PA 66 (Europe-Africa-Middle East) LNP* VERTON* RX03013 is a compound based on PA 66 resin containing Long Glass Fiber, Proprietary Lubricant. Added features include: Internally Lubricated. |
|||
Tensile Modulus | 12.5 - 14.0 GPa | 1810 - 2030 ksi | ISO 527 |
Vyncolit 2923 W Novolac Phenolic Mineral filled phenolic molding compound with excellent heat resistance and dimensional stability.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Tensile Modulus | 12.5 - 14.0 GPa | 1810 - 2030 ksi | ISO 527 |
Vyncolit 2723 W Novolac Phenolic Mineral and organic filled phenolic molding compound with excellent mechanical, thermal and dielectric properties. I2/FO classified under NF F 16-101 (Fire & Smoke classification).USES: Circuit bre.. |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 GVZ 45 HWCP 45% Glass Fiber Nylon 6, Impact Resistant, Good Surface Finish, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600 MZ 401 CP Combination Nylon 66, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TSGL-50-4 nat PA666-GF50 Product description: Grilon TSGL-50/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 50% long glass fibers. Grilon TSGL-50/4 natural is characterized by the following .. |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4107 nat PA612-GF40 Product description: Grilamid XE 4107 natural is a 40% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4107 are: low water absorptiong.. |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612
(Unverified Data**) 43% Glass Reinforced Polyamide 612Zytel 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | 1 mm/min; ISO 527 |
Eurostar Starflam RF0097P PA66/6, 45% Glass Filled, Injection Molded Starflam RF0097P is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1009Z270EM)Information provided by Polym.. |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | ISO 527 |
Eurotec® Tecomid® NB40 GR30 NL AX70 PA6, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® T1 GF 30 (3466) PPA Dry, 30% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Tensile Modulus | 12.5 GPa @Temperature -40.0 °C |
1810 ksi @Temperature -40.0 °F |
ISO Data |
BASF Petra® 130 FR BK-112 30% Glass Filled PET Petra 130 FR BK-112 is a 30% glass fiber reinforced, black pigmented, flame retardant injection molding compound based on post-consumer and post-industrial recycle polyethylene erephthalate feedstoc.. |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | same value from ASTM and ISO test. |
BASF Capron® GR40 40% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron GR40 is a 40% glass reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensional stability. It is also ava.. |
|||
Tensile Modulus | 12.5 GPa @Temperature 23.0 °C |
1810 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612
(Unverified Data**) Zytel® 77G43L BK031 is a 43% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Verton UV007S PPA LNP VERTON* UV007S is a compound based on Polyphthalamide resin containing Long Glass, Long Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP .. |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | |
LATI Latilub 88/50-20GRT K/10 PEEK, 10% Carbon Fiber Reinforced, Graphite/PTFE Filled Self-lubricating product based on Polyetheretherketone (PEEK). Graphite / PTFE. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provid.. |