Polymer Property : Tensile Modulus = 11.6 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 11.6 GPa
1680 ksi
ASTM D638
Oxford Polymers 40GF 40% Glass Fiber Filled Polycarbonate for Injection Molding
40% Glass Fiber Filled Polycarbonate for Injection MoldingInformation provided by Oxford Polymers.
Tensile Modulus 11.6 GPa

@Temperature 23.0 °C
1680 ksi

@Temperature 73.4 °F
ISO 527-2/1
PolyOne Bergamid™ A70 G30 U Polyamide 66 (Nylon 66)
Information provided by PolyOne
Tensile Modulus 11.6 GPa

@Temperature 23.0 °C
1680 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® HTN 52G35HSL BK083 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTN52G35HSL BK083 is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds. It is also a PPA resin.Information provid..
Tensile Modulus 11.6 GPa
1680 ksi
ISO 527
Solvay Specialty Polymers Amodel® A-1340 HS Polyphthalamide (PPA) Resin, 40% Mineral/Glass Reinforced, Dry as Molded &a
AMODEL® A-1340 HS is a 40% mineral/glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, high tensile strength and low warpage..
Tensile Modulus 11.6 GPa
1680 ksi
Idemitsu Kosan Xarec® EA 537 SPS, 30% Glass Filled
Crystalline Polymer, Glass Filled, Ignition Resistant, Impact Modified. Used in Electronic and Electrical applications
Tensile Modulus 11.6 GPa
1680 ksi
ISO 527-1/-2
Kuraray Genestarâ„¢ G1352A-M41 Nylon, 35% Glass Filled
Low friction reinforced injection grade.Main Features:Low friction coefficientAbrasion resistanceExamples of applications:Friction and wear applicationGear and wheel
Tensile Modulus 11.6 GPa
1680 ksi
ISO 527 Type 1A
Solvay TECHNYLSTARâ„¢ SX 216 V50 PA6, 50% glass filled, Conditioned
Description: TECHNYLSTAR Polyamide, reinforced with 50% of glass fiber, characterized by a high fluidity of the melt, for injection molding.Available in: Asia Pacific, Europe and North America Produ..
Tensile Modulus 11.6 GPa
1680 ksi
ISO 527 Type 1A
Solvay TECHNYLSTARâ„¢ SX 218 V50 PA6, 50% glass filled, Conditioned
Description: TECHNYLSTARâ„¢ SX 218 V50 is based on a patented high flow polyamide 6 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. This product i..
Tensile Modulus 11.6 GPa
1680 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics ULTEM SF2350 PEI Blend
High flow Ultem blends for thin wall application
Tensile Modulus 11.6 GPa
1680 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics ULTEM SF2350 PEI Blend (Asia Pacific)
High flow Ultem blends for thin wall application
Tensile Modulus 11.6 GPa
1680 ksi
5 mm/min; ASTM D 638
SABIC Innovative Plastics Ultem SF2350 PEI Blend (Europe-Africa-Middle East)
High flow Ultem blends for thin wall applicationThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Tensile Modulus 11.6 GPa
1680 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Valox® ENH4565 PBT (Asia Pacific)
33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE.
Tensile Modulus 11.6 GPa
1680 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP UF006AS PPA
LNP THERMOCOMP* UF006AS is a compound based on Polyphthalamide resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized.
Tensile Modulus 11.6 GPa
1680 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Valox® EXVX1403 PBT (Asia Pacific)
33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE.
Tensile Modulus 11.6 GPa
1680 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Valox® IQNH4565 PBT (Asia Pacific)
Valox* iQNH4565 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 29% based on EPEAT..
Tensile Modulus 11.6 GPa
1680 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP PF008QS PA 6
LNP THERMOCOMP* PF008QS is a compound based on Nylon 6 resin containing 40% Glass Fiber. Added features of this material include: Heat Stabilized, Reduced Moisture.
Tensile Modulus 11.6 GPa
1680 ksi
ASTM D638
Plenco 3303 Phenolic, Granular, Compression Molded
Plenco 03303 is a renumber of Plaslok 5303. Plenco 03303 is a two-stage, mineral and flock-filled phenolic molding compound offering excellent electrical insulating properties. It can be processed b..
Tensile Modulus 11.6 GPa
1680 ksi
ASTM D638
Westlake Plastics Zelux® 40% GF Polycarbonate 40% Glass Filled
Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and ..
Tensile Modulus 11.6 GPa
1680 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® BG-40 FC PA6-GF40
Product description: Grilon BG-40 FC is a heat stabilized PA6 injection molding grade with 40% glass fibers. Grilon BG-40 FC has the following important properties: High stiffnessExcellent surface f..
Tensile Modulus 11.6 GPa
1680 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® BG-40 S PA6-GF40
Product description: Grilon BG-40 S is a normal viscosity PA 6 injection molding type with 40% glass fibers. Grilon BG-40 S has the following important properties: High stiffnessExcellent surface fi..
Tensile Modulus 11.6 GPa
1680 ksi
ISO 527-1/-2
DuPont Performance Polymers Crastin® SK695FR NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
30% Glass Reinforced Flame Retardant Polybutylene Terephthalate  Crastin® SK695FR is a 30% glass reinforced flame retardant polybutylene terephthalate for injection moulding.Information provided b..
Tensile Modulus 11.6 GPa
1680 ksi
1 mm/min; ISO 527
Eurostar Starflam PF0023E PA6, Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam PF0023E is a Mineral Flame Retardant, Halogen Free, Red Phosphorous Free, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Tensile Modulus 11.6 GPa

@Temperature -40.0 °C
1680 ksi

@Temperature -40.0 °F
ISO Data
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Conditioned)
Ultramid 8233G HS is a heat stabilized, 33% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also..
Tensile Modulus 11.6 GPa
1680 ksi
ISO 527-2
Ascend Performance Materials Vydyne® R535 Nylon 66, 35% Glass Reinforced, DAM
Vydyne® R535 is general-purpose, hydrolysis-resistant, 35% glass-fiber reinforced PA66 resin. This product is lubricated for improved flow and offers superior surface appearance. Glass-reinforced V..
Tensile Modulus 11.6 GPa
1680 ksi
ISO 527-2
Ascend Performance Materials Vydyne® R535H NT651 Nylon 66, 35% Glass Reinforced, DAM
Vydyne® R535H NT651 is 35% glass-fiber reinforced PA66 resin. Available in natural, it is heat-stabilized with an electrically neutral heat stabilizer. It is designed specially for electrical appli..
Tensile Modulus 11.6 GPa
1680 ksi
1[mm/min]; ISO 527-1/2
Akro-Plastic Akromid® A3 GF 35 (2421) PA 6.6 Dry, 35% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
Tensile Modulus 11.6 GPa
1680 ksi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® HTN 52G35HSL BK083 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced PPA High Performance Polyamide Zytel HTN52G35HSL BK083 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin that can be molded in water heated m..
Tensile Modulus 11.6 GPa
1680 ksi
ASTM D638
LNP Thermocomp® UF-1006 A HS Polyphthalamide, Glass Fiber Reinforcement  (discontinued **)