Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 11.5 GPa | 1670 ksi | ISO 527-1/-2 |
DSM Akulon® S223-G8U (Dry) 43% Glass Reinforced Nylon 66 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | ISO 527-1/-2 |
DSM Akulon® Ultraflow™ K-FKGS6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry)
(discontinued ** The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | d.a.m.; ISO 527-1, -2; 1 mm/min |
Lanxess Durethan® AKV 35 HR H2.0 901510 Nylon 66, Glass Fiber Reinforced PA 66, 35% glass fibers, injection molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | 1 mm/min; ISO 527-1,-2 |
Lanxess Durethan® AKV 35 LT H3.0 000000 Nylon 66, 35% Glass Fiber PA 66, 35% glass fiberInformation provided by LANXESS. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | ISO 527-1/-2 |
Lanxess Durethan® BKV 140 H2.0 900051 Copolyamide, 40% Glass Fiber CoPA, injection molding grade, 40% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 40, even in.. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 2400 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 2400F PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 listing. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be.. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 2410 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® ENH4565 PBT (Asia Pacific) 33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem HU2400 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | ISO 527-1/-2 |
DSM Arnite® B427 SE/R PBT-GF35 FR(17) 35% Glass Reinforced, Flame Retardant |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4120 black 9916 PA*-GF30 Product description: Grivory XE 4120 black 9916 is a 30% glass fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolya.. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Rynite® FR530 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont .. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612
(Unverified Data**) 43% Glass Reinforced Polyamide 612Zytel 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® HTN 51G35HSLR BK420 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G35HSLR BK420 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin with improved hydrolysis resistance.. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® HTN 51G35HSLR BK420J Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide with Improved Surface Appearance Zytel HTN51G35HSLR BK420J is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin w.. |
|||
Tensile Modulus | 11.5 GPa @Temperature 23.0 °C |
1670 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® HTN 51G35NOX BK420 Polyphthalamide (PPA) Zytel® HTN51G35NOX BK083 is a 35% glass reinforced high performance polyamide resin developed for Selective Catalytic Reduction applications that require exposure to water/urea solution. It is also.. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | ISO 527 |
Eurotec® Tecodur® PB70 GR30 NL XA 21 PBT/PET 30% glass fiber reinforced, UL94 V0 Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | ISO 527 |
Eurotec® Tecomid® NT40 GR30 NL XA60 PPA, 30% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural Information provided by Eurotec® |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® BG-50 H PA6-GF50 Product description: Grilon BG-50 H is a high heat stabilized PA6 injection molding grade with 50% glass fibers. Grilon BG-50 H has the following important properties: High stiffnessHigh heat resist.. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | ISO 527 |
Eurotec® Tecopet® PT70 GR30 NL100 PS20 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural, fast crystallization grade Information provided by Eurotec® |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | 1mm/min; ISO 527 |
BASF Ultradur B 4406 G6 Q113 30% Glass Filled PBT Ultradur B4406 G6 Q113 is an UL V0 injection molding, PBT grade with 30% glass fiber reinforcement. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | 1mm/min; ISO 527 |
BASF Ultradur B 4406 G6 Q717 30% Glass Filled PBT Ultradur B 4406 G6 Q717 is an UL V0 injection molding, PBT grade with 30% glass fiber reinforcement. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | ISO 527-1/-2 |
DSM Akulon® K-FKGS6 (Dry) 30% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Rynite® FR530L NC010 Polyethylene Terephthalate (PET) Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | ISO 527-2 |
Solvay Specialty Polymers Amodel® A-1933 HSL Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1933 HSL is a 33% glass reinforced grade of polyphthalamide (PPA) resin. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment. Thi.. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® BG-50 FC PA6-GF50 Product description: Grilon BG-50 FC is a heat stabilized PA6 injection molding grade with 50% glass fibers. Grilon BG-50 FC has the following important properties: Short cycle timesExcellent surfac.. |
|||
Tensile Modulus | 11.5 GPa | 1670 ksi | ASTM D638 |
LNP Thermocomp® SPS-F-1006 HS Syndiotactic Polystyrene, Glass Fiber Reinforcement
(discontinued **) Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti.. |