Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 11.41 GPa
1655 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON DEF42 PC
LNP STAT-KON* DEF42 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Electrically Conductive.
Tensile Modulus 11.41 GPa
1655 ksi
ASTM D638
Plenco 50130 PET, Pellet, Injection Molded, Black  (discontinued **)
PLENCO 50130 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in natural and black.Informat..