Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 10.9 GPa | 1580 ksi | |
Plastcom SLOVAMID 66 GF 25 FRA 5 PA66, 25% glass fibre, flame retardant FeaturesPA 66 for injection moulding, reinforced with 25% glass fibre and halogen flame retardant. Application in electrical industry: breakers, coilforms, covers, terminals. Slightly decreased flam.. |
|||
Tensile Modulus | 10.9 GPa @Temperature 23.0 °C |
1580 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 74G33W NC010 Nylon 66
(Unverified Data**) Zytel® 74G33W NC010 is a 33% glass reinforced nylon 66 and nylon 6 co-melt resin with improved weatherability.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 10.9 GPa | 1580 ksi | ISO 527-1/-2 |
Kuraray Genestarâ„¢ GC1201A-M41 Nylon, Glass Filled and Carbon Filled Reinforced injection grade for conductive applications.Main Features:ConductivityHeat resistanceChemical resistanceExample of applications:Quick connector |
|||
Tensile Modulus | 10.9 GPa | 1580 ksi | ISO 527-2 |
Solvay Specialty Polymers Amodel® A-8422 LS WH159 Polyphthalamide (PPA), 22% Mineral Amodel® A-8422 LS is a light-stabilized, high-reflectivity, 22%-reinforced white polyphthalamide (PPA) that exhibits high heat resistance, high strength and stiffness over a broad temperature ran.. |
|||
Tensile Modulus | 10.9 GPa | 1580 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP LF006EL PEEK (Europe-Africa-Middle East) LNP* THERMOCOMP* LF006EL is a compound based on Polyetheretherketone resin containing Glass Fiber. Added features include: Easy Molding. FDA Compliant Raw Materials. |
|||
Tensile Modulus | 10.9 GPa | 1580 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP PFB55 PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PFB55 is a compound based on PA 6 resin containing Glass Bead, Glass Fiber. |
|||
Tensile Modulus | 10.9 GPa | 1580 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP QF00A PA 6/10 (Europe-Africa-Middle East) LNP* Thermocomp* QF00A is a compound based on Nylon 6/10 resin containing Glass Fiber. |
|||
Tensile Modulus | 10.9 GPa | 1580 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-kon RE003 PA 66 (Europe-Africa-Middle East) LNP* Stat-kon* RE003 is a compound based on Nylon 66 resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 10.9 GPa | 1580 ksi | ASTM D638 |
Plenco 3509 Phenolic, Granular, Transfer Molded PLENCO 03509 is a mineral and flock filled phenolic molding compound offering excellent electrical properties, dimensional stability, and improved heat resistance. UL recognized under component file.. |
|||
Tensile Modulus | 10.9 GPa | 1580 ksi | ASTM D638 |
Plenco 4466 Phenolic, Granular, Compression Molded PLENCO 04466 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength and cosmetic properties. UL recognized under component file E40654. 04466.. |
|||
Tensile Modulus | 10.9 GPa | 1580 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 74G33W NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced UV Stabilized Polyamide 66 + Polyamide 6 Zytel 74G33W NC010 is a 33% glass reinforced nylon 66 and nylon 6 co-melt resin with improved weatherability.Information provided by DuP.. |
|||
Tensile Modulus | 10.9 GPa | 1580 ksi | |
Radici Radilon® A RV330 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Tensile Modulus | 10.9 GPa | 1580 ksi | After 7 days in boiling water |
Gharda Chemicals GAFONE™ 3430GF PES, Glass Fiber-Reinforced
(discontinued **) Glass fiber reinforced granules for injection molding. With lower viscosity for molding intricate cross sections.Characteristics: Very high rigidityGood dielectric propertiesHigh mechanical strengt.. |
|||
Tensile Modulus | 10.9 GPa | 1580 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON PX06418 PA 6 LNP* VERTON* PX06418 is a compound based on Nylon 6 containing proprietary fillers. Added features of this grade are: Heat Stabilized, Structural. |