Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 10.56 GPa | 1532 ksi | ASTM D638 |
Plenco 50030 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 50030 is an engineering grade glass reinforced polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in white, natural, and black.Information sup.. |
|||
Tensile Modulus | 10.56 GPa | 1532 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON OEP32 PPS - Linear (Asia Pacific) LNP* STAT-KON* OEP32 is a compound based on PPS - Linear resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 10.56 GPa | 1532 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON OEP32 PPS - Linear LNP STAT-KON* OEP32 is a compound based on PPS - Linear resin containing 10% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear Resistant. |