Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.983 GPa @Temperature -20.0 °C |
287.6 ksi @Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® BM6450XD BK560 Polybutylene Terephthalate (PBT)