Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.979 GPa @Temperature 120 °C |
287.0 ksi @Temperature 248 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 80G14A NC010A Nylon 66