Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.60 GPa | 232 ksi | |
Plastcom SLOVALEN PC 79 T 20 PP/C reinforced with 20% mineral filler Features: Modified PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal. Decreased shrinkage. Antistatic agent. Delivered in natural mode and i.. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | STN EN ISO 527-2 |
Plastcom SLOVASTYR® E BT N PET Basic type PET for injection molding, modified for general use, with excellent manufacturing properties. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fast.. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | ISO 527-1/-2 |
Quadrant EPP Symalit® 1000 ECTFE, unfilled, lining industries (ISO Data) Symalit 1000 ECTFE is made from a fluoropolymer resin that is a copolymer of ethylene and chlorotrifluoroethylene. It exhibits good mechanical properties combined with an excellent chemical resistan.. |
|||
Tensile Modulus | 1.60 GPa @Temperature 23.0 °C |
232 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
PolyOne Bergamid™ A70 white Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® A 30 S 000000 Nylon 66 PA 66 standard injection molding-grade, non-reinforced, good demolding, very rapid solidificationApplication Examples: plug connectors, terminal blocks, cable clips, bobbins |
|||
Tensile Modulus | 1.60 - 1.70 GPa @Thickness 2.00 mm |
232 - 247 ksi @Thickness 0.0787 in |
1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 6020 Polyvinylidene Fluoride (PVDF) Solef® 6020 PVDF homopolymer has very high viscosity for membranes and lithium batteries. It is available exclusively as powder.Features: Homopolymer; Ultra High ViscosityUses: Batteries; Membran.. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | ISO 527 |
Styrolution PS 2710 HIPS Styrolution PS 2710 is a high impact grade of polystyrene with improved stress crack resistance, developed for extrusion and thermoforming applications, especially for the refrigerator industry.Impr.. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | 1mm/min; ISO 527 |
Styrolution Terblend® N NM-11 ABS/PA6 (Conditioned) Terblend N NM-11 is an ABS/PA6 blend combining very high impact strength, even at low temperatures, with an excellent processability and surface appearance.Information provided by STYROLUTION, which.. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | 1mm/min; ISO 527 |
Styrolution Terblend® N NM-13 ABS/PA6 (Dry) Terblend N NM-13 is a new experimental ABS/PA6-Blend with improved impact strength at low temperatures. It can be easily processed on any standard injection molding machine.Information provided by .. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | 1mm/min; ISO 527-2 |
Borealis Daplen™ EF210AE Polypropylene TPO Compound Daplen™ EF210AE is a 20% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q.. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | 1mm/min; ISO 527-2 |
Borealis HC600TF Polypropylene HC600TF is a polypropylene homopolymer intended for thermoformed packaging applications. Its very good organoleptic properties allows this grade to be used with any masterbatch without discoloring .. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | ISO 527-2 |
Total PPC 10641 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 10641 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 44 g/10 min.Polypropylene PPC 10641 is characterized by high fluidity with good mechanical prope.. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | ISO 527-2 |
Total PPH 10060 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 10060 homopolymer. PPH 10060 is characterized by high fluidity and is particularly suitable for injection molding applications. The material provides a good balance betwe.. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | ISO 527-2 |
Total PSI 8350 High Impact Polystyrene 8350 is a very high impact polystyrene for extrusion. This grade has an improved environmental stress crack resistance in comparison with standard high impact grades. It is proposed for the produc.. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | ISO 527-2 |
Total PPC 13442 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 13442 is a nucleated antistatic heterophasic copolymer. PPC 13442 is characterized by very high fluidity with good mechanical properties. It has been formulated for excellent ant.. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | MD; ASTM D882 |
Eastman Eastar A150 Copolyester, Film Eastar A150 Copolyester is a poly(1,4-cyclohexylene-dimethylene terephthalate/isophthalate). It is produced by reacting terephthalic acid and isophthalic acid with the glycol 1,4-cyclohexanedimethan.. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® L 25 LM PA12 Product Description: Grilamid L 25 LM is a heat and UV stabilized nylon 12 grade for tube extrusion. According to DIN 73378 Grilamid L 25 LM corresponds to the type PA 12 HL. Grilamid L 25 LM fulfil.. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TR 90 LS PAMACM12 Product description: Grilamid TR 90 LS natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 90 LS natural contains a processing a.. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® ST820 BK503 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Polybutylene Terephthalate with Excellent Impact Resistance Crastin ST820 BK503 is an unreinforced Super Tough black polybutylene terephthalate resin for injection molding.Information p.. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 132F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 132F NC010 is a nucleated lubricated polyamide 66 for injection molding. It was developed for fast production cycles and high productivity applications.Info.. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | ASTM D638 |
Aclo Accucomp ABS ABS812L High Impact Grade |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | ASTM D638 |
Azdel SuperLite® SL550800-100 PP Resin Matrix / 55% Glass Fiber (3.5 mm Molded Thickness) AZDEL SuperLite® SL550800-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0334C20L1 Calcium Reinforced |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | ASTM D638 |
Azdel SuperLite® SL551000-100 PP Resin Matrix / 55% Glass Fiber (4.5 mm Molded Thickness) AZDEL SuperLite® SL551000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | |
BASF Novolen® 2240 P Polypropylene Nucleated grade for injection moldings.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | cond; ISO 527-1/-2 |
DSM Akulon® K225-KV PA6 FR(30) Flame Retardant (Halogen free), Heat stabilized |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | Secant; ISO527-2/1 |
ExxonMobil PP7064L1 Polypropylene Impact Copolymer Product Description: A nucleated impact copolymer resin with medium flow, high stiffness and antistatic properties. It is suitable for molding applications like consumer products, closures, contain.. |