Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.50 GPa | 218 ksi | |
Plastcom SLOVALEN PC 18 FRT 5 PP, mod. of mech. properties, fire retardant FeaturesModified copolymer PP for extrusion, contains the modifier of mechanical properties and non halogen and free phosphor flame retardant. Delivered in natural mode and in the full RAL colour sc.. |
|||
Tensile Modulus | 1.50 GPa @Temperature 23.0 °C |
218 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
PolyOne Bergamid™ B700 UF black Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl RF1132 PPE+PP PPE+PP blend for high frequency applications. Good heat resistance and low DK.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | ISO 527-1/-2 |
Styrolution Styrolux® 684 D SBC Description: Styrolux® 684 D is a clear styrene-butadiene copolymer (SBC) used in injection molding for parts with enhanced toughness as well as in sheet and film extrusion and blow molding. Part.. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL PX1185 PPE+HIPS (Europe-Africa-Middle East) NORYL PX1185 is a special NORYL grade developed for extrusion of automotive trims. NORYL PX1185 offers high heat resistance and good impact performance. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER (Asia Pacific) PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 216 NATURAL FA PA66, Conditioned Description: Unreinforced polyamide 66, medium viscosity, for injection molding.Available in: EuropeProduct Applications: TECHNYL® A 216 Natural FA offers all of the primary properties of unreinf.. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | 1mm/min; ISO 527-2 |
Borealis BH374MO Polypropylene Copolymer BH374MO is a heterophasic copolymer. This grade is characterized by optimum combination of very high stiffness, good flow properties and good impact strength. Products molded with this grade exhibi.. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | 1mm/min; ISO 527-2 |
Borealis Daplen™ EE340AE Polypropylene TPO Compound Daplen™ EE340AE is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q.. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | 1mm/min; ISO 527-2 |
Borealis HD120MO Polypropylene HD120MO is a polypropylene homopolymer with a good combination of mechanical properties intended for injection molding. Applications: sanitary equipment, caps and closures, and general packagingInf.. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | At 1 mm/min; ISO 527-2 |
Borealis Bormod™ BF970MO Polypropylene for Injection Molding Bormod BF970MO is a heterophasic copolymer characterized by an optimum combination of very high stiffness and high impact strength.Bormod BF970MO is a new generation grade for very fast production o.. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | At 1 mm/min; ISO 527-2 |
Borealis Daplen™ ED213AE TPO Compound Daplen ED213AE is a 20% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen ED213AE is a material with excellent impact/ stiffness ratio. Thanks to its low.. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | ISO 527-1/-2 |
DSM Akulon® S223-DH Nylon 66 (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | ISO 527-1/-2 |
DSM Akulon® S223-DK Nylon 66 (European Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 20 H FR PA12 FR Product Description: Grilamid L 20 H FR is a flame retarded, medium viscosity product, based on Polyamide 12 (PA12). Grilamid L 20 H FR contains no halogen or phosphorus, it has a light natural colo.. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | ISO 527-2/1 |
ExxonMobil PP1013H1 Polypropylene Homopolymer Product Description: A homopolymer resin that meets certified requirements for use in Medical and Pharmaceutical applications.Availability: Europe and North America Features:Autoclave SterilizableE.. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | ISO 527-2 |
Domo 1101P Polypropylene Homopolymer Information provided by Domo. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | ISO 527-2 |
Domo 1101S Polypropylene Homopolymer Information provided by Domo. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | ISO 527-2 |
Domo 1102J Polypropylene Homopolymer Information provided by Domo. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® RS LC1201 BK040A Nylon 1010
(Unverified Data**) Toughened Renewably Sourced Medium Viscosity Polyamide 1010 Developed for Extrusion Zytel RS LC1201 BK040A is a renewably sourced polyamide 1010 resin containing a minimum of 85% renewably sourced i.. |
|||
Tensile Modulus | 1.50 GPa | 217 ksi | ASTM D790 |
Clariant Renol ABNN732017 Nylon 6 with anchored silicone Data provided by Clariant Masterbatches |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 157HSL BK010 Nylon 612
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 612 Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | ISO 527-2 |
Domo 1100L Polypropylene Homopolymer Information provided by Domo. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | ISO 527 |
Eurotec® Tecomid® NA40 NL IH PA6.6, impact modified, natural Information provided by Eurotec® |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | |
BASF Novolen® 1100 L Polypropylene, Injection Molding Grade Injection molded parts, film tape, fibrillated film and monofilaments.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOTUF W1000I PBT (Europe-Africa-Middle East) LNP* THERMOTUF* W1000I is a compound based on Polybutylene Terephalate resin. Added features include: High Impact |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | |
Plastcom SLOVALEN PH 91 C 20 PP, 20% mineral filling FeaturesModified homopolymer and copolymer PP for injection moulding with the contenct of 20% microground, chemically modified talc. Increased strength, rigidity and thermal application up to 100°C.. |