Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.44 GPa | 209 ksi | ISO 527-1/-2 |
Kuraray Genestarâ„¢ N1006D-H31 Nylon Standard unreinforced extrusion grade. Main Features:Chemical resistanceLong term heat resistanceExample of applications:Tube applications |
|||
Tensile Modulus | 1.44 GPa | 209 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON SX90398 PA 12 LNP STAT-KON* SX90398 is a compound based on Nylon 12 resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Tensile Modulus | 1.44 GPa | 209 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics XYLEX FXY330DF PC+POLYESTER Polyester+PC alloy. Diffusion Effect. Color package may affect performance. |
|||
Tensile Modulus | 1.44 GPa | 209 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics XYLEX FXY330DF PC+POLYESTER (Europe-Africa-Middle East) Polyester+PC alloy. Diffusion Effect. Color package may affect performance. |
|||
Tensile Modulus | 1.44 GPa | 209 ksi | ISO527-2/1 |
ExxonMobil AP03B Polypropylene Impact Copolymer Product Description: A high crystallinity, medium impact copolymer resin with high melt flow rate and excellent processing attributes. It is designed for injection molded large appliance applicatio.. |
|||
Tensile Modulus | 1.44 GPa | 209 ksi | ISO527-2/1A/1 |
ExxonMobil PP5032E3 Polypropylene Copolymer Product Description: A polypropylene homopolymer type designed for production of monofilaments, tapes for the textile industry, geo textiles, fibrillated tapes for ropes and twines in the packaging.. |
|||
Tensile Modulus | 1.44 GPa | 209 ksi | Conditioned 15 days at 23°C - 50% RH; ISO 527 |
Arkema Group Rilsamid® PA 12 AESNO MED Nylon 12 Rilsamid® AESNO MED is a rigid polyamide 12 with high viscosity designed for tube extrusion. This grade dedicated to extrusion offers the highest quality and it is specifically designed to meet the.. |
|||
Tensile Modulus | 1.44 GPa | 209 ksi | 1 mm/min |
Arkema Group Rilsan® BECN TL Nylon 11, Sheathing Grade (Conditioned) Designation ISO 1874-PA11,KHL,12-010Rigid grade for sheathing of wires and cables. Available color: natural. Light and heat stabilized.High abrasion resistance. Well adapted melt viscosity. Ability .. |
|||
Tensile Modulus | 1.44 GPa | 209 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics XYLEX FXY330DF PC+POLYESTER (Asia Pacific) Polyester+PC alloy. Diffusion Effect. Color package may affect performance. |