Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.38 GPa | 200 ksi | TM R050-36 |
Resinlab® EP1287 Filled, Flame Retardant Epoxy Syntactic Foam Resinlab™ EP1287 is a two part filled, flame retardant epoxy syntactic foam. It utilizes glass microspheres to reduce cured density and improve machinability. This product will be self-extinguishin.. |
|||
Tensile Modulus | 1.38 GPa | 200 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ AS-000/15T Acrylonitrile Butadiene Styrene (ABS) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Modulus | 1.38 GPa | 200 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ ATT-000/5T Black Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Modulus | 1.38 GPa | 200 ksi | ASTM Data |
Americas Styrenics Styron® 6187SF High Impact Polystyrene
(discontinued **) STYRON® 6187SF structural foam molding resin is a high impact polystyrene grade with proprietary ignition resistance additive package to achieve UL 94 V-0 rating. It offers excellent moldability an.. |
|||
Tensile Modulus | 1.38 GPa | 200 ksi | |
Ineos Styrenics Polystyrene 476M Q598 (NAFTA) High-impact grade of polystyrene with good ESCR designed to provide uniform melt flow for excellent processability.Information provided by BASF.Ineos Styrenics purchased this product line from BASF .. |
|||
Tensile Modulus | 1.38 GPa | 200 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM STM1600 PEI Copolymer (Europe-Africa-Middle East) Siltem 1600 is a flexible copolymer designed for wire and cable applications. It offers a halogen free (according VDE 0472) flame retardant solution that also offers low smoke emission and toxicity... |
|||
Tensile Modulus | 1.38 GPa | 200 ksi | |
Saint-Gobain Rulon® DC1042 Bearing/Seal PTFE Can be used in a wide range of sealing and bearing applications. Rulon DC1042 is ideal for applications in which the bearing, seal is in contact with harsh chemicals or in applications where electri.. |
|||
Tensile Modulus | 1.38 GPa | 200 ksi | ASTM D638 |
ScanTube PVDF Tubing Information provided by ScanTube, Inc. |
|||
Tensile Modulus | 1.38 GPa | 200 ksi | ASTM D638 |
Lubrizol Hipscon™ M-530 Static Control Polystyrene Hipscon™ M-530 is a conductive, carbon black filled, polystyrene available as extruded sheet and compound. Thermoformed trays are lightweight and easily formed into deep pockets that maintain unif.. |
|||
Tensile Modulus | 1.38 - 1.72 GPa @Temperature 23.9 °C |
200 - 250 ksi @Temperature 75.0 °F |
|
Master Bond EP21TDCHTND Versatile, toughened two component epoxy for bonding, sealing and coating Product Description: Master Bond EP21TDCHTND is a two component epoxy adhesive, sealant and coating featuring high performance, versatility and exceptional user friendliness. It has a very forgiving.. |
|||
Tensile Modulus | >= 1.38 GPa | >= 200 ksi | |
Master Bond LED401 White One Part, LED Curable Compound Description: Master Bond LED401 White is a one part LED type system that cures fully upon exposure to a 405 nm wavelength light source where the presence of any UV light is minimal or incidental. In.. |
|||
Tensile Modulus | 1.38 - 1.72 GPa | 200 - 250 ksi | |
Master Bond MB306 Low Viscosity Methyl Cyanoacrylate Features superior bonding properties. Master Bond MB306 is a single component, low viscosity, rapid setting, methyl cyanoacrylate adhesive. Similar to other types of “super glue”, MB306 cures ver.. |
|||
Tensile Modulus | >= 1.38 GPa | >= 200 ksi | |
Master Bond UV10TKLO-2 UV Curable Compound for Aerospace Applications Description: Master Bond UV10TKLO-2 is a special one component UV curable epoxy modified system for high performance bonding, sealing and encapsulation. This system has passed rigorous testing to me.. |
|||
Tensile Modulus | 1.38 GPa | 200 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® RS 3061HSL BK039A Nylon 610
(Unverified Data**) Unreinforced Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3061HSL BK039A is a renewably sourced polyamide 610 resin containing a minimum of 60% renewably sourced ingredie.. |
|||
Tensile Modulus | 1.38 GPa | 200 ksi | 1 mm/min |
Arkema Group Rilsan® AMN Y TLD Nylon 12, MoS2 Filled (Conditioned) Designation ISO 1874-PA12,MHLS,14-010,MD05Grade with molybdenum filler for injection molding. Available color: steel gray. Light and heat stabilized. Mold-release agent.Low friction coefficient. Goo.. |
|||
Tensile Modulus | 1.38 GPa | 200 ksi | ASTM D638 |
Quadrant EPP Semitron® ESd 225, Extruded, Static Dissipative Acetal (ASTM Product Data Sheet) |
|||
Tensile Modulus | 1.38 GPa | 200 ksi | ISO 527 |
Premix Thermoplastics PRE-ELEC® ESD 12-000
(discontinued **) PRE-ELEC ESD 12-000 is a static dissipative thermoplastic compound based on polyacetal copolymer. The dissipative property is permanent and built into the polymer chain. The products made out of PRE.. |
|||
Tensile Modulus | 1.38 GPa | 200 ksi | TM R050-36 |
Resinlab® EP1026HP Epoxy Adhesive Resinlab™ EP1026HP is a high performance fast setting epoxy adhesive designed for bonding metals, ceramics, glass and most plastics. This product gives good resistance to water salt spray, inorgan.. |
|||
Tensile Modulus | 1.38 GPa | 200 ksi | TM R050-36 |
Resinlab® EP1300 Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP1300 Black (Formerly Lab Product W092602) is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It has a pot life of about one hour and .. |