Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.24 GPa | 180 ksi | 100 micron film; ASTM D882 |
Kaneka PHBH Rigid Bio-based Polymer A copolymer produced of 3-hydroxybutyrate and 3-hydroxyhexanoate produced by fermentation of plant oils. It has excellent biodegradability (under anaerobic, aerobic, aquatic, and compost conditions.. |
|||
Tensile Modulus | 1.24 GPa | 180 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP FL004 PE LNP* Lubricomp* FL004 is a compound based on Polyethylene resin containing 20% PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 1.24 GPa | 180 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP TH0300B PU LNP* Thermocomp* Th0300B is a compound based on Polyurethane containing proprietary fillers. Characteristics of this grade are High Specific Gravity. |
|||
Tensile Modulus | 1.24 GPa | 180 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PPX PPX7115 PPE+PP High modulus/impact/heat PPE+PP |
|||
Tensile Modulus | 1.24 GPa | 180 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PPX PPX7115 PPE+PP (Asia Pacific) High modulus/impact/heat PPE+PP. |
|||
Tensile Modulus | 1.24 GPa | 180 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PPX PPX7115F PPE+PP High modulus/impact/heat PPE+PP. Compliant with US FDA food contact regulations for temperatures of use of room temperature and below. |
|||
Tensile Modulus | 1.24 GPa | 180 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed. |
|||
Tensile Modulus | 1.24 GPa | 180 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS (Asia Pacific) PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed. |
|||
Tensile Modulus | 1.24 GPa | 180 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS (Europe-Africa-Middle East) PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed. |
|||
Tensile Modulus | 1.24 GPa | 180 ksi | ASTM D638 |
Lubrizol Stat-Rite® M-690 Static Control PETG Alloy Stat-Rite® M-690 is a static dissipative PETG alloy. Stat-Rite® M-690 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protectio.. |
|||
Tensile Modulus | >= 1.24 GPa | >= 180 ksi | |
Master Bond UV24TKLO One Component, UV-Curable, Low Outgassing Adhesive System Master Bond Polymer System UV24TKLO is a one part UV curable epoxy modified formulation for bonding, sealing and encapsulation. It passes the rigorous requirements for low outgassing as per ASTM E-5.. |
|||
Tensile Modulus | 1.24 GPa | 180 ksi | ASTM D638 |
Total PPC M6823MZ Metallocene Isostatic Propylene Polymer TOTAL Petrochemicals Polypropylene M6823MZ is an isostatic form of copolymer polypropylene made via TOTAL Petrochemicals proprietary metallocene catalyst technology.Clarity. M6823MZ incorporates th.. |
|||
Tensile Modulus | 1.24 GPa | 180 ksi | ASTM D638 |
Total PPH 3727W Polypropylene, High Performance Injection Molding Grade Balanced Properties TOTAL Polypropylene 3727W strikes an optimum balance between excellent mechanical properties (tensile, flex and impact) and processability making it a superior molding grade for.. |
|||
Tensile Modulus | 1.24 GPa | 180 ksi | Secant; ISO 527-2 |
ExxonMobil Exxtral™ BMU 131 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance, good surface appearance and good weatherability designed for automotive exterior .. |
|||
Tensile Modulus | 1.24 GPa | 180 ksi | 1 mm/min |
Arkema Group Rilsan® ARVO 950 TLD Nylon 12, Rotomolding Grade (Dry) Designation ISO 1874-PA12,RHLR,16-010Grade for rotomolding. Available color: natural. Light and heat stabilized. Mold-release agent.Easy to be processed in the same conditions as polyethylene. High .. |
|||
Tensile Modulus | 1.24 GPa | 180 ksi | ASTM D638 |
Azdel SuperLite® SL550700-100 PP Resin Matrix / 55% Glass Fiber (3.5 mm Molded Thickness) AZDEL SuperLite® SL550700-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Tensile Modulus | 1.24 GPa | 180 ksi | ASTM D638 |
Americas Styrenics EC6600 High Impact Polystyrene Product CharacteristicsExcellent printabilityMatte surface finishHigh heat distortion temperatureGood low temperature toughnessFood Contact CompliantTypical ApplicationsLithographic sheetPrinted toy.. |
|||
Tensile Modulus | 1.24 GPa | 180 ksi | ASTM D638 |
Aclo Accutech Polypropylene HP0315V Homopolymer High Heat Approved to GMP.PP.013 |
|||
Tensile Modulus | 1.24 GPa | 180 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® UR-20GF/000 Thermoplastic Elastomer - TPU, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |