Tensile Modulus 1.227 GPa
178.0 ksi
Y-Direction; ASTM D638
SpinTech Veritexâ„¢ Shape Memory Polymer Composite
Veritexâ„¢ is a fiber-reinforced composite that uses a shape memory polymer, VeriflexÂ, as the matrix. This allows Veritex to easily change shape above its activation temperature. At lower tempe..