Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.17 GPa | 170 ksi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ DP-9162-3 Polypropylene, Unspecified (PP, Unspecified) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Tensile Modulus | 1.17 GPa | 170 ksi | ASTM D638 |
Flint Hills P6G2Z-090 Impact Copolymer Polypropylene Features: Excellent impact strength and weldability. Product does not contain animal derived components.Applications: Injection Molding and thermoforming - Automotive coolant bottlesInformation p.. |
|||
Tensile Modulus | 1.17 GPa | 170 ksi | ASTM D638 |
Laurel BioComposite Bio-Resâ„¢ 20% Composite in HDPE Bio-Resâ„¢ can be blended with various resins in certain applications. It can be included at rates up to 40% in manufactured plastic products while maintaining or enhancing the desired characteri.. |
|||
Tensile Modulus | 1.17 GPa | 170 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY 63000CTC PC+POLYESTER (Asia Pacific) A permanent antistatic PC-Alloy compound that features transparency and superior cleanliness for advanced semiconductor packaging applications |
|||
Tensile Modulus | 1.17 GPa | 170 ksi | 2 in/min; ASTM Test |
Styrolution Styrolux 3G55 SBC Styrolux 3G55 is a thermoplastic styrene-butadiene block copolymer which is suitable for film and sheet extrusion, and thermoforming. It offers and outstanding combination of crystal clarity and ex.. |
|||
Tensile Modulus | 1.17 GPa | 170 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP TH0450C PU LNP* Thermocomp* TH0450C is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Tensile Modulus | 1.17 GPa | 170 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP TH0450C PUR (Asia Pacific) LNP* Thermocomp* TH0450C is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Tensile Modulus | 1.17 GPa | 170 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PPX PPX7112 PPE+PP PPE+PP blend. Suitable for painted exterior automotive applications. |
|||
Tensile Modulus | 1.17 GPa | 170 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PPX PPX7112 PPE+PP (Asia Pacific) PPE+PP blend. Suitable for painted exterior automotive applications. |
|||
Tensile Modulus | 1.17 GPa | 170 ksi | ASTM D638 |
Westlake Plastics Propylux® Void-Free Polypropylene Propylux is made from polypropylene resin. Among its most notable characteristics are its mechanical toughness, chemical resistance and resistance to abrasion. These properties make it suitable fo.. |
|||
Tensile Modulus | 1.17 GPa | 170 ksi | ASTM D638 |
Total PPR 6827MZ Polypropylene, Random Copolymer - High Flow Clarified - for Injection Molding Clarity. TOTAL Polypropylene 6827MZ exhibits superior clarity and produces molded parts with improved impact compared with parts molded from homopolymer polypropylene.Antistat. 6827MZ contains an a.. |
|||
Tensile Modulus | 1.17 GPa | 170 ksi | 2 in/min; ASTM D638 |
ExxonMobil HDPE HYA 800 High Density Polyethylene Resin Product Description: HYA 800 is a homopolymer HDPE grade, characterized by high stiffness, high rigidity and high flow.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Thermal .. |
|||
Tensile Modulus | 1.17 GPa | 170 ksi | ASTM D638 |
Ensinger Tecapeek® XP-104 Compression Molded PEEK Compound, with 7% Molybdenum Disulfide, 3% PTFE and 25% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Tensile Modulus | 1.17 GPa | 170 ksi | 1 mm/min |
Arkema Group Rilsan® AMN D Nylon 12, Rigid, Injection Grade (Conditioned) Designation ISO 1874-PA12,MR,14-010Rigid grade for injection molding. Available colors: black, natural, orange, red and white. Possibilities of heat and light stabilizing agents. Mold-release agent... |
|||
Tensile Modulus | 1.17 GPa | 170 ksi | 1 mm/min |
Arkema Group Rilsan® AMV TL Nylon 12, Rigid, Injection Grade (Dry) Designation ISO 1874-PA12,MHLR,16-010Rigid grade for injection molding. Available color: natural. Light and heat stabilized. Mold-release agent.High impact strength. Easy filling of the mold due to .. |
|||
Tensile Modulus | 1.17 GPa | 170 ksi | Conditioned 15 days at 23°C - 50% RH; ISO 527 |
Arkema Group Rilsamid® PA 12 AMNO MED Nylon 12 Rilsamid® AMNO MED is a thermoplastic polyamide 12. This grade dedicated to injection offers the highest quality and it is specifically designed to meet the stringent requirements of the medical ap.. |
|||
Tensile Modulus | 1.17 GPa | 170 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON MS000IL PP LNP* STAT-KON* MS000IL is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: High Impact, Low Extractible, Electrically Conductive, food c.. |