Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.10 GPa | 160 ksi | STN EN ISO 527-2 |
Plastcom PLASTALEN® PQ 81 T 15/1 Polypropylene reinforced with mineral filler, impact modified Modified PP for injection molding with the content of 15% mineral filler. Application in automotive industry. Delivered in black grade.Information Provided by Plastcom spol. s r.o. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | |
Radici Radilon® S 32HS (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Tensile Modulus | 1.10 GPa @Temperature 23.0 °C |
160 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
PolyOne Bergamid™ B700 Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Tensile Modulus | 1.10 GPa @Temperature 23.0 °C |
160 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
PolyOne Bergamid™ B700 X2 Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ FR PE 152 Polyethylene, Unspecified (PE, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | |
LyondellBasell Lupolen® 5231 HX HDPE, Impact Grade Medium flow, impact resistant, very stress-crack resistant grade for closures, bottles that contain carbonated liquids, storage and tote boxes, as well as engineering components.Data was collected b.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | ASTM D638 |
Ineos Styrenics Polystyrene 486N (NAFTA) High-impact grade of polystyrene with excellent ESCR.Information provided by BASF.Ineos Styrenics purchased this product line from BASF in 2005. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® B 30 S FN40 000000 Nylon 6 PA 6, injection molding grade, non- reinforced, good flowability, easy-release, fast cycling, UL 94V-2 off 0,75 mm, GWIT 775°C bei 0,75/1,5mm |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | ISO 527-2 |
Solvay Specialty Polymers Polidan® T/A Polyethylene, Crosslinked (XLPE) POLIDAN® T/A is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Features.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | ASTM D638 |
Lubrizol Stat-Rite® S-680 Static Control PETG Alloy Stat-Rite® S-680 is a static dissipative PETG alloy. Stat-Rite® M-680 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protectio.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | 1mm/min; ISO 527-3 |
Borealis RE420MO Polypropylene Random Copolymer, Transparent RE420MO is a specially modified highly-transparent polypropylene random copolymer with medium melt flow rate. This grade is intended for injection molding and stretch blow molding. and is designed .. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | TD; ASTM D882-A |
Borealis FS1470 High Density Polyethylene FS1470 is a high density polyethylene film grade which combine excellent extrusion behavior with superior mechanical properties. Films made of FS1470 have high impact and tensile strength, and bala.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | ISO 527-2 |
Total PPC 4660 Polypropylene, Heterophasic Copolymer ATOFINA Polypropylene PPC 4660 is heterophasic copolymer. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | |
Covestro Bayflex® 110-50 Polyurethane Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® FG 40 NL nat 6025 PA6 Product description: Grilon FG 40 NL natural 6025 is a modified, high viscosity polyamide 6. Compared to conventional polyamide 6 Grilon FG40 NL natural 6025 offers the following improvements:Better.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 16 LM PA12 Product Description: Grilamid L 16 LM is a , low viscosity extrusion type, based on Polyamide 12 (PA12). Grilamid L 16 LM is UV- and heat stabilized. The modification with a nucleation agent results.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 20 GM PA12 Product Description: Grilamid L 20 GM is a medium viscosity, heat stabilized polyamide 12 non-reinforced injection molding grade. This product has very good flow characteristics. Special features of.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 20 L PA12 Product Description: Grilamid L 20 L is a medium viscosity Polyamide 12 (PA12) extrusion type. It is UV and heat stabilized. Its main features are: High surface quality Very good UV and heat resista.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 25H FWA black 9225 PA12 Product Description: Grilamid L 25 H FWA black 9225 is a highviscosity, unreinforced and heat stabilized Polyamide 12 (PA12). Grilamid L 25 H FWA black 9225 is designed for technical injection mould.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | Foaming Direction |
Cymat A35620SC 030SS Stabilized Aluminum Foam Description: Cymat A35620SC 030SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.3 g/cm3. The mechanical properties of SAF make it .. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | ISO527-2 |
ExxonMobil PPU0009F Polypropylene Impact Copolymer Product Description: An unstabilized impact copolymer resin designed for automotive and compounding applications.Availability: Europe Processing Method: CompoundingInformation provided by ExxonMobi.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 CP Nylon 6, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 20H FWA nat PA12 Product Description: Grilamid L 20 H FWA natural is a medium viscosity, unreinforced and heat stabilized Polyamide 12 (PA12). Grilamid L 20 H FWA natural is used for technical injection molded parts.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 25 LM PA12 Product Description: Grilamid L 25 LM is a heat and UV stabilized nylon 12 grade for tube extrusion. According to DIN 73378 Grilamid L 25 LM corresponds to the type PA 12 HL. Grilamid L 25 LM fulfil.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 444AHS BK152 Nylon 66
(Unverified Data**) Toughened Heat Stabilized Polyamide 66 Zytel 444AHS is a toughened heat stabilized black polyamide 66 resin for injection molding. It is a high flow processing friendly material.Information provided.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® A3 (2414) PA 6.6 Conditioned AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | |
BASF Novolen® 3240 NC Polypropylene Grade containing nucleating agent for transparent injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | cond.; ISO 527 |
Azoty Tarnow™ Tarnamid® T-29 MCS Polyamide 6 - Colored Colored medium-high viscosity grade for injection molding.Tarnamid® has the following main properties:High mechanical strength, rigidity and hardnessHigh impact strengthHigh vibration damping capac.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | STN EN ISO 527-2 |
Plastcom SLOVALEN PQ 51 N Polypropylene Homopolymer, Modified with Elastomer, Impacted FeaturesHomopolymer PP modified with elastomer. The addition of thermoplastic elastomer causes increased toughness, possible alternative to PP copolymers. General application in all industry branc.. |
|||
Tensile Modulus | 1.10 GPa @Temperature 150 °C |
160 ksi @Temperature 302 °F |
ISO 527-2 |
Solvay Specialty Polymers Amodel® A-1240 L Polyphthalamide (PPA)
(discontinued **) Amodel A-1240 L is a 40% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten.. |