Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.825 GPa | 120 ksi | ISO 527-1/-2 |
Quadrant EPP TIVAR® 1000 EC PE-UHMW + specific additives (ISO Data) TIVAR 1000 EC is a PE-UHMW grade containing specific additives rendering this material a lower surface resistivity than TIVAR 1000 antistatic, improving electrical conductivity and UV-resistance |