Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.735 GPa | 107 ksi | ISO 527-1 |
Iran Petrochemical (PCC) MF3713 High Density Polyethylene MF3713 is a high molecular weight high density polyethylene.Applications: bags, products for use in property modification.Information provided by Iran Petrochemical Commercial Co. |