Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.450 - 0.750 GPa | 65.3 - 109 ksi | ASTM D638 |
Manifattura Cattaneo PTFE Polytetrafluoroethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Tensile Modulus | 0.450 - 0.550 GPa | 65.3 - 79.8 ksi | ISO 527-2 |
Borealis BD212CF Polypropylene Copolymer BD212CF is a heterophasic copolymer. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: BD212CF is designed for food packaging, l.. |
|||
Tensile Modulus | 0.450 - 0.550 GPa | 65.3 - 79.8 ksi | ISO 527-2 |
Borealis BD712CF Polypropylene Copolymer BD712CF is a heterophasic copolymer. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: BD712CF is recommended for food packaging.. |
|||
Tensile Modulus | 0.450 GPa | 65.3 ksi | ISO 527-2 |
Borealis Borsoft™ SF203CF Soft Polypropylene Copolymer for Extrusion Coating Borsoft SF203CF is a new statistic-heterophasic propylene-ethylene copolymer suitable for coating applications. Its polymer structure permits perfect adhesion to certain products. According to the.. |
|||
Tensile Modulus | 0.450 GPa | 65.3 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® 2S 25 W 20 HL X black 9992 PA610 Product Description: Grilamid 2S 25 W 20 HL X black 9992 is a semi-flexible high viscosity heat stabilized, impact modified and plasticized Polyamide 610, especially suitable for extrusion applicati.. |
|||
Tensile Modulus | 0.450 GPa | 65.3 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® 2S 25 W 20 HL X nat PA610 Product Description: Grilamid 2S 25 W 20 HL X natural is a semi-flexible high viscosity heat and UV stabilized, impact modified and plasticized Polyamide 610, espcailly suitable for extrusion applic.. |
|||
Tensile Modulus | 0.450 GPa | 65.3 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® 2S 25 W 20 X black 9992 PA610-I Product Description: GRILAMID 2S 25 W 20 X black 9992 is a semi-flexible high viscosity heat and impact modified polyamide 610, especially suitable for extrusion applications. This PA610 product is .. |
|||
Tensile Modulus | 0.450 GPa | 65.3 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® 2S 25 W 20 X nat PA610-I Product Description: GRILAMID 2S 25 W 20 X natural is a semi-flexible high viscosity heat and UV stabilized, impact modified polyamide 610, especially suitable for extrusion applications. This PA610.. |
|||
Tensile Modulus | 0.450 GPa | 65.3 ksi | Foaming Direction |
Cymat A35620SC 020SS Stabilized Aluminum Foam Description: Cymat A35620SC 020SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.2 g/cm3. The mechanical properties of SAF make it .. |
|||
Tensile Modulus | 0.450 GPa | 65.3 ksi | 1 mm/min; ISO 527 |
Eurostar Starpylen HU 70E3 HDPE, Injection Molding Starpylen HU 70E3 is a High Density Polypropylene Injection Molding Resin (also known as HU70E3)Information provided by Eurostar. |
|||
Tensile Modulus | 0.450 GPa | 65.3 ksi | 1 mm/min; ISO 527 |
Eurostar Starpylen MH0200A HDPE, Injection Molding Starpylen MH0200A is a High Density Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 0.450 GPa | 65.3 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 25 W 20 X PA12-I Product Description: Grilamid L 25 W 20 X is a semi-flexible plasticized high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 20 X is impact modified and UV and heat stabilized. Th.. |
|||
Tensile Modulus | 0.450 GPa | 65.3 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® L 25 W 20 X PA12-I Product Description: Grilamid L 25 W 20 X is a semi-flexible plasticized high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 20 X is impact modified and UV and heat stabilized. Th.. |
|||
Tensile Modulus | 0.450 GPa | 65.3 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® L 25 W 40 PA12 Product Description: Grilamid L 25 W 40 is a flexible, plasticised, high viscosity extrusion grade of Polyamide 12 (PA12) Grilamid L 25 W 40 is UV and heat stabilized. The main features of Grilamid .. |
|||
Tensile Modulus | 0.450 GPa | 65.3 ksi | MD; ASTM D882-A |
Borealis Borstar® FB4370 Medium Density Polyethylene Borstar® FB4370 is a linear medium density polyethylene grade combining excellent extrusion properties with high film stiffness. Applications: Borstar® FB4370 has been developed especially for ap.. |