Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.340 GPa | 49.3 ksi | 1mm/min; DIN 53457 |
Advanced Elastomer Systems VistaFlex® 912-B Thermoplastic Rubber
(discontinued **) Description: A black super high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as .. |
|||
Tensile Modulus | 0.340 GPa | 49.3 ksi | TD; ASTM D882-A |
Borealis Borstar® FB3450 HDPE for Film Extrusion Borstar® FB3450 is a high density polyethylene. Borstar® FB3450 is well suited for multilayer coextruded films where higher stiffness and toughness than in standard LDPE and LLDPE is required. Ap.. |
|||
Tensile Modulus | 0.340 GPa | 49.3 ksi | Bending Modulus; ASTM D790 |
UBE UMERIT 2500F Metallocene LLDPE Description: UBE Super Polyethylene Umerit® is an ethylene-olefin copolymer made by UBE using the metallocene catalytic method. The metallocene catalytic method results in superior physical propert.. |
|||
Tensile Modulus | 0.340 GPa @Temperature 23.0 °C |
49.3 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Hytrel® HTR8241 TPC-ET
(Unverified Data**) Hytrel® HTR8241 is a 65 nom.Shore D, non discoloring stabilizer, plasticiser free high performance resin for extrusion; high viscosity; outstanding mechanical properties up to 120°C and excellent .. |