Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.303 GPa | 43.9 ksi | at yield; chs 2.0 in/min; ASTM D638 |
Diamond Polymers GPPS BEADS Injection Molding Grade, General Purpose Polystyrene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Modulus | 0.303 GPa | 43.9 ksi | at yield; chs 2.0 in/min; ASTM D638 |
Diamond Polymers NPS80-1800B Injection Molding Grade, General Purpose Polystyrene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |