Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.230 GPa @Temperature 23.0 °C |
33.4 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Hytrel® DYM250S BK472 TPC-ET
(Unverified Data**) Hytrel® DYM250S BK472 is a medium modulus resin suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 49D and contains fine particle size carbon black.In.. |
|||
Tensile Modulus | 0.230 GPa | 33.4 ksi | ISO 527 |
FKuR Kunststoff Bio-Flex® F 1110 Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Tensile Modulus | 0.230 GPa | 33.4 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP YL003 Polyester Elastomer LNP* LUBRICOMP* YL003 is a compoudn based on Polyester Elastomer resin containing 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Tensile Modulus | 0.230 GPa | 33.4 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP TH0300A PUR LNP THERMOCOMP* TH0300A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Tensile Modulus | 0.230 GPa | 33.4 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP TH0300A PUR (Asia Pacific) LNP THERMOCOMP* TH0300A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Tensile Modulus | 0.230 GPa | 33.4 ksi | MD; ASTM D882-A |
Borealis FT5230 Low Density Polyethylene FT5230 is a Low Density Polyethylene for Film Extrusion. This grade is developed for the production of packaging film with good optical properties for medium duty film applications. Applications: .. |
|||
Tensile Modulus | 0.230 GPa | 33.4 ksi | MD; ASTM D882-A |
Borealis FT5231 Low Density Polyethylene FT5231 is a Low Density Polyethylene for blown film. Tubular technology. Contains Antioxidant. This grade is developed for the production of packaging film with good optical properties for medium d.. |
|||
Tensile Modulus | 0.230 GPa | 33.4 ksi | MD; ASTM D882-A |
Borealis FT5232 Low Density Polyethylene FT5232 is a Low Density Polyethylene for Film Extrusion. Tubular Technology. Includes medium slip additive and antioxidant. This grade is developed for the production of packaging film with good op.. |
|||
Tensile Modulus | 0.230 GPa | 33.4 ksi | MD; ASTM D882-A |
Borealis FT5236 Low Density Polyethylene FT5236 is a Low Density Polyethylene for Film Extrusion. Tubular Technology. Includes anti-block, antioxidant and medium slip additives. Applications FT5236 has been developed especially for applic.. |
|||
Tensile Modulus | 0.230 GPa | 33.4 ksi | Bending Modulus; ASTM D790 |
UBE UMERIT 613A Metallocene LLDPE Description: UBE Super Polyethylene Umerit® is an ethylene-olefin copolymer made by UBE using the metallocene catalytic method. The metallocene catalytic method results in superior physical propert.. |
|||
Tensile Modulus | 0.230 GPa | 33.4 ksi | Through Plane Direction |
Cymat A35620SC 020SS Stabilized Aluminum Foam Description: Cymat A35620SC 020SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.2 g/cm3. The mechanical properties of SAF make it .. |
|||
Tensile Modulus | 0.230 GPa @Temperature 80.0 °C |
33.4 ksi @Temperature 176 °F |
ISO Data |
BASF Ultramid® 8254 HS BK-102 PA6 (Conditioned) Ultramid 8254 HS is a highly flexible, heat stabilized, impact modified nylon 6 extrusion grade for tubing applications. |
|||
Tensile Modulus | 0.230 GPa | 33.4 ksi | average; in the plane; ISO 527 1-2 |
3A Composites Core Materials AIREX® C70.250 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible .. |
|||
Tensile Modulus | 0.230 GPa | 33.4 ksi | average; perpendicular to plane; ASTM C297 |
3A Composites Core Materials AIREX® T92.200 Easy Processing Structural Foam AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable, UV r.. |
|||
Tensile Modulus | 0.230 GPa | 33.4 ksi | ISO 527-1/-2 |
DSM Arnitel® CM622 TPC-ES 60 Shore D, Extrusion |
|||
Tensile Modulus | 0.230 GPa | 33.4 ksi | ASTM D638 |
Elastomer Engineering Elastamide 400 Elastomer Modified RIM Nylon 6 18% crystallinity. Information supplied by Elastomer Engineering. |