Mechanical Properties Metric English Comments
Tensile Modulus 0.225 GPa
32.6 ksi
ISO 527-1/-2
DSM Arnitel® EB500 50 Shore D, Blow Molding Grade Copolyester Elastomer (North America)  (discontinued **)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Modulus 0.225 GPa
32.6 ksi
ISO 527-1/-2
DSM Arnitel® EB500 Polyether Ester Elastomer (European and Asian Grade)  (discontinued **)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Modulus 0.225 GPa
32.6 ksi
ISO 527