Polymer Property : Tensile Modulus = 0.0420 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.0420 GPa
6.09 ksi
1 mm/min
Arkema Group Pebax® MX 1059 Polyether Block Amide (PEBA) (Conditioned)
POLYETHER BLOCK AMIDE (PEBA) Hardness 35 shore D Good resistance to oils. Applications: Automotive, cable...ISO data provided by the manufacturer, Arkema.
Tensile Modulus 0.0420 GPa
6.09 ksi
average; in the plane; ISO 527 1-2
3A Composites Core Materials AIREX® C71.55 Elevated Temperature Structural Foam
AIREX® C71 is a closed cell, crosslinked polymer foam especially formulated to maintain its stability also at higher processing or service temperatures. It combines excellent stiffness and strength..