Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.0159 GPa | 2.30 ksi | Molded Properties; ISO 527-2/1 |
ExxonMobil Escorene™ FL 00728CC Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00728CC is an excellent coextrusion partner in extrusion coating, blown and cast film. Good adhesion onto OPP in coextrusion. This grade offers excellent optical, low gel and.. |
|||
Tensile Modulus | 0.0159 GPa | 2.30 ksi | Molded Properties; ISO 527-2 |
ExxonMobil Escorene™ UL 00328 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 00328 is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: No Applications: Compoun.. |
|||
Tensile Modulus | 0.0159 GPa | 2.30 ksi | Molded Properties; ISO 527-2/1 |
ExxonMobil Escorene™ UL 00728 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 00728 is a copolymer of ethylene and vinyl acetate.Processing Conditions: Processing temperatures above 220°C (428°F) may cause resin degradation.Availability: Africa & Mid.. |
|||
Tensile Modulus | 0.0159 GPa | 2.30 ksi | Molded Properties; ISO 527-2/1 |
ExxonMobil Escorene™ UL 00728CC Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 00728CC is a copolymer of ethylene and vinyl acetate.Processing Conditions: Processing temperatures above 220°C (428°F) may cause resin degradation.Availability: Africa & M.. |
|||
Tensile Modulus | 0.0159 GPa | 2.30 ksi | Molded Properties; ISO 527-2/1 |
ExxonMobil Escorene™ UL 00728FF Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 00728 is a copolymer of ethylene and vinyl acetate.Processing Conditions: Processing temperatures above 220°C (428°F) may cause resin degradation.Availability: Africa & Mid.. |
|||
Tensile Modulus | 0.0159 GPa | 2.30 ksi | (0.2 in/min), Molded Properties; ASTM D638 |
ExxonMobil Escorene™ UL 02528CC Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 02528CC is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: YesFree .. |
|||
Tensile Modulus | 0.0159 GPa | 2.30 ksi | Molded Properties; ISO 527-2/1 |
ExxonMobil Escorene™ FL 00328 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00328 is a copolymer of ethylene and vinyl acetate offering low gel. Processing Conditions: Processing temperatures above 220°C (428°F) may cause resin degradation. Machine.. |