Polymer Property : Tensile Modulus = 0.00150 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.00150 GPa
0.217 ksi
ASTM D412
Aearo E-A-R Specialty Composites VersaDamp™ V-2350 TPE
VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded..
Tensile Modulus 0.00150 GPa
0.217 ksi
ASTM D412
Aearo E-A-R Specialty Composites VersaDamp™ V-2375 TPE
VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded..